MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arlon Electronic Materials 25FR Low-Cost Ceramic Hydrocarbon
Categories: Polymer; Thermoset

Material Notes: High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit Boards

  • Low loss ceramic-filled thermoset resin
  • Tight dielectric tolerance control
  • Excellent dimensional stability
  • Excellent price/performance ratio

Benefits:

  • Greater signal integrity
  • Wider eye patterns
  • Excellent dimensional stability
  • Utilizes standard FR-4 processes
  • Excellent thermal properties

Typical Applications:

  • Cellular Base Station Antennas, Power Amplifiers, Down Converters
  • High Speed Backplanes

Information provided by ARLON Electronic Materials.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ASTM D792 Method A
Water Absorption 0.090 %0.090 %IPC TM-650 2.6.2.1
Thickness 99.1 microns3.90 milPrepreg thickness - glass style 1080
 147 microns5.80 milPrepreg thickness - glass style 2112
 170 microns6.70 milPrepreg thickness - glass style 2313
Outgassing - Total Mass Loss  0.070 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.070 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
Water Vapor Recovered; ASTM E595-90
 0.24 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.24 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
ASTM E595-90
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.00 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
ASTM E595-90
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 96.5 MPa14000 psiASTM D882
Flexural Strength 241.48 MPa35024 psiASTM D790
Peel Strength 0.877 kN/m5.00 pliAfter Thermal Stress; IPC TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.17e+14 ohm-cm4.17e+14 ohm-cmCondition A; IPC TM-650 2.5.17.1
Surface Resistance 8.90e+14 ohm8.90e+14 ohmCondition A; IPC TM-650 2.5.17.1
Dielectric Constant 3.58
@Frequency 1e+10 Hz
3.58
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Dissipation Factor 0.0035
@Frequency 1e+10 Hz
0.0035
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C8.89 µin/in-°Fx, before Tg; IPC TM-650 2.4.24
 18.0 µm/m-°C10.0 µin/in-°Fy, before Tg; IPC TM-650 2.4.24
CTE, linear, Transverse to Flow 59.0 µm/m-°C32.8 µin/in-°Fz, before Tg; IPC TM-650 2.4.24
Thermal Conductivity 0.450 W/m-K
@Temperature 100 °C
3.12 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1225
Flammability, UL94 V-0V-0
 
Descriptive Properties
Temperature Coefficient of Dielectric (ppm/°C)50IPC TM-650 2.5.5.5 adapted (-10 - 140°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance
BASF Ultraform® H 4320 Q600 POM
Rogers Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System
Celanese Celanex® 2300 GV1/50 PBT, 50% Glass Reinforced

PARLM9872 / 149025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.