MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0019 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0051 cm/cmISO 294-4, 2577
Melt Flow 36 g/10 min
@Load 5.00 kg,
Temperature 270 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 210 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 16000 MPaISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
 
Descriptive Properties
AdditivesRelease agent
FeaturesHeat stabilized or stable to heat
FormPellets
ISO Short NameISO1874-PA6, MHR, 10-160, GF50
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, DRY
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Domo TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Celanese Zytel® 73G50HSLA BK416 PA6-GF50
Celanese Zytel® 73G30HSL BK416 PA6-GF30

PLANX0784 / 98999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.