MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183/A
Water Absorption 1.05 %
@Temperature 23.0 °C,
Time 86400 sec
1.05 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  30 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 464 °F
 30 cP
@Shear Rate 10000 1/s,
Temperature 250 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 482 °F
 30 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 500 °F
 150 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
150 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
 190 cP
@Shear Rate 1000 1/s,
Temperature 250 °C
190 cP
@Shear Rate 1000 1/s,
Temperature 482 °F
 200 cP
@Shear Rate 1000 1/s,
Temperature 240 °C
200 cP
@Shear Rate 1000 1/s,
Temperature 464 °F
 300 cP
@Shear Rate 100 1/s,
Temperature 260 °C
300 cP
@Shear Rate 100 1/s,
Temperature 500 °F
 400 cP
@Shear Rate 100 1/s,
Temperature 250 °C
400 cP
@Shear Rate 100 1/s,
Temperature 482 °F
 500 cP
@Shear Rate 100 1/s,
Temperature 240 °C
500 cP
@Shear Rate 100 1/s,
Temperature 464 °F
Linear Mold Shrinkage 0.0043 cm/cm0.0043 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psiASTM D638
 190 MPa27600 psiISO 527 Type 1A
Tensile Stress at Strain  60.0 MPa
@Strain 0.5 %
8700 psi
@Strain 0.5 %
 100 MPa
@Strain 1 %
14500 psi
@Strain 1 %
 160 MPa
@Strain 2 %
23200 psi
@Strain 2 %
 180 MPa
@Strain 3 %
26100 psi
@Strain 3 %
Elongation at Break 3.2 %3.2 %ISO 527 Type 1A
 3.5 %3.5 %ASTM D638
Tensile Modulus 9.60 GPa1390 ksiISO 527 Type 1A
Flexural Strength 255 MPa37000 psiISO 178
Flexural Modulus 8.40 GPa1220 ksiISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180/1eA
 125 kJ/m²59.5 ft-lb/in²ASTM D256
Charpy Impact Unnotched 9.20 J/cm²43.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.83.8IEC 60250
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 475 V475 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
17.8 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75/Af
Flammability, UL94 HB
@Thickness 0.400 - 3.20 mm
HB
@Thickness 0.0157 - 0.126 in
1210
Oxygen Index 23 %23 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 - 3.20 mm
1200 °F
@Thickness 0.0630 - 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-245°C
Mixing Zone245-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned
Domo TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Domo Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6

PRHOD767 / 137998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.