MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.

Available in: Asia Pacific, Europe and North America

Product Applications: TECHNYLSTAR TM SX 216 V50 is suitable for all applications where a high rigidity is required. Due to its outstanding flow properties, the material easily fills the mould and the surface aspect of the finished part is excellent. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183/A
Water Absorption 0.72 %
@Temperature 23.0 °C,
Time 86400 sec
0.72 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0072 cm/cm0.0072 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0023 cm/cm0.0023 in/in
Linear Mold Shrinkage, Transverse 0.0032 cm/cm0.0032 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psiISO 527 Type 1A
Elongation at Break 2.6 %2.6 %ISO 527 Type 1A
Tensile Modulus 17.0 GPa2470 ksiISO 527 Type 1A
Flexural Modulus 15.5 GPa2250 ksiISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1eA
Izod Impact, Unnotched (ISO) 90.0 kJ/m²42.8 ft-lb/in²ISO 180/1eU
Charpy Impact Unnotched 8.50 J/cm²40.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 V500 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 220 - 225 °C428 - 437 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone240-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Envalior Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber
Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled
Domo TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0

PRHOD840 / 138071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.