MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: TECHNYLSTAR™ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product is available in black color.

Benefits: Due to its outstanding flow characteristics, the product allows more freedom in mould and part design versus a standard polyamide solutions.

Available in: Asia Pacific, Europe and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: It is used in a wide variety of industries. The product is particularly suitable for all applications where a high rigidity is required.

Product data for dry samples.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183/A
Water Absorption 0.72 %
@Temperature 23.0 °C,
Time 86400 sec
0.72 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  100 cP
@Shear Rate 1000 1/s,
Temperature 270 °C
100 cP
@Shear Rate 1000 1/s,
Temperature 518 °F
 110 cP
@Shear Rate 1000 1/s,
Temperature 250 °C
110 cP
@Shear Rate 1000 1/s,
Temperature 482 °F
 140 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
140 cP
@Shear Rate 1000 1/s,
Temperature 446 °F
 220 cP
@Shear Rate 100 1/s,
Temperature 270 °C
220 cP
@Shear Rate 100 1/s,
Temperature 518 °F
 300 cP
@Shear Rate 100 1/s,
Temperature 250 °C
300 cP
@Shear Rate 100 1/s,
Temperature 482 °F
 400 cP
@Shear Rate 100 1/s,
Temperature 230 °C
400 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Linear Mold Shrinkage 0.0076 cm/cm0.0076 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0025 cm/cm0.0025 in/in
Linear Mold Shrinkage, Transverse 0.0033 cm/cm0.0033 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psiISO 527 Type 1A
Tensile Stress at Strain  25.0 MPa
@Strain 0.5 %
3630 psi
@Strain 0.5 %
 140 MPa
@Strain 1 %
20300 psi
@Strain 1 %
 210 MPa
@Strain 2 %
30500 psi
@Strain 2 %
Elongation at Break 2.5 %2.5 %ASTM D638
 2.6 %2.6 %ISO 527 Type 1A
Tensile Modulus 17.0 GPa2470 ksiISO 527 Type 1A
Flexural Strength 320 MPa46400 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiASTM D790
 15.5 GPa2250 ksiISO 178
Izod Impact, Notched 1.80 J/cm3.37 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1eA
Izod Impact, Unnotched (ISO) 90.0 kJ/m²42.8 ft-lb/in²ISO 180/1eU
Charpy Impact Unnotched 8.50 J/cm²40.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75/Af
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone240-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 60 H2.0 EF DUS060 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, DRY
Domo TechnylStar™ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY
Domo TechnylStar™ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY
Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled

PRHOD847 / 138078

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.