MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 13RM19 Strip Steel
Categories: Metal; Ferrous Metal; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik 13RM19 is a stainless spring steel combining high mechanical strength with a non-magnetic structure. This combination of properties has previously been found mainly in expensive Co-Ni-base or Cu-Be-alloys. The corrosion resistance is comparable to that of ASTM 301.

Sandvik 13RM19 is characterized by:

  • non-magnetic structure in all conditions
  • high mechanical strength in the cold rolled condition. The strength can be further increased without any effect on the non-magnetic structure by tempering.
  • high elastic limit and energy storing capacity in the cold rolled and tempered condition

Sandvik 13RM19 also possesses good fatigue properties and excellent ductility, which makes it a most suitable choice for springs and other high strength applications where ferromagnetic materials cannot be used.

Service temperature: up to 250°C (480°F)

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 850 MPa
@Thickness 0.0300 - 4.00 mm
annealed
 1300 MPa
@Thickness 0.0200 - 2.80 mm
cold rolled
 1500 MPa
@Thickness 0.0150 - 1.90 mm
cold rolled
 1100 MPa
@Diameter 0.0300 - 4.00 mm
cold rolled
 1600 MPa
@Diameter 0.0150 - 0.900 mm
cold rolled
Tensile Strength, Yield 470 MPa
@Strain 2 %
annealed
 1020 MPa
@Strain 2 %
cold rolled and tempered
Modulus of Elasticity 190 GPa
Fatigue Strength <= 1000 MPacold rolled; limit, fluctuating tensile strength
 <= 1070 MPacold rolled and tempered, 480°C/ 2 hours; limit, fluctuating tensile strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000700 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
 17.0 µm/m-°C
@Temperature 30.0 - 200 °C
 18.0 µm/m-°C
@Temperature 30.0 - 300 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 16.0 W/m-K
@Temperature 100 °C
 19.0 W/m-K
@Temperature 300 °C
Maximum Service Temperature, Air 250 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.11 %
Chromium, Cr 18.5 %
Iron, Fe 67 %as balance
Manganese, Mn 6.0 %
Nickel, Ni 7.0 %
Nitrogen, N 0.25 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.80 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium, Ti
CuMoCu 13/74/13
ERG Aerospace Duocel® Silicon Carbide Foam
Overview of materials for Copper Alloy
ASTM A228 Steel (UNS K08500)

NSANDV279 / 19173

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.