MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP820 Acrylic Adhesives
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability and bond well to many metals, ceramics, wood and most plastics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 45000 cPAccelerator
 70000 cPBase
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
Elongation at Break 50 - 75 %ASTM D882
Shear Strength 300 psiOverlap, Aluminum -solvent cleaned only
 300 psiOverlap, CRS/CRS tested after 120°C/2 wks
 700 psiOverlap, Fiberglass Reinforced Plastic
 850 psiOverlap, CRS/CRS tested after 90°C/2 wks/90% RH
 850 psiOverlap, CRS/CRS tested after tap water 1 wk/RT
 1000 psiOverlap, Etched Alum, 93°C/100% RH/2 wks
 1000 psiOverlap, ABS
 1150 psiOverlap, Polycarbonate
 1150 psiOverlap, CRS (oily) 49°C/100% RH/2 wks
 1200 psiOverlap, Galvanized Steel
 1200 psiOverlap, Fir Wood
 1250 psiOverlap, Acrylic
 1350 psiOverlap, CRS/CRS after 7 days of Immersion in IPA
 1500 psiOverlap, CRS/CRS after 7 days of Immersion in Gasoline
 1500 psiOverlap, FR-4/FR-4 tested after tap water 1 wk/RT
 1600 psiOverlap, FR-4/FR-4 tested after 90°C/2 wks/90% RH
 1650 psiOverlap, Etched Alum (oily) 49°C/100% RH/4 wks
 1750 psiOverlap, PVC
 1950 psiOverlap, CRS/CRS after 7 days of Immersion in Machine Oil
 2000 psiOverlap, FR-4 Glass Epoxy
 2000 psiOverlap, FR-4/FR-4 tested after RT aging
 2400 psiOverlap, Cold Rolled Steel (oily)
 2500 psiOverlap, Cold Rolled Steel
 2500 psiOverlap, Control
 2500 psiOverlap, CRS/CRS tested after RT aging
 2900 psiOverlap, Aluminum -etched/oily
 3100 psiOverlap, Aluminum -120 frit sandpaper
 3200 psiOverlap, Aluminum-etched
 3300 psiOverlap, FR-4/FR-4 tested after 120°C/2 wks
 1450 psi
@Temperature 93.0 °C
Overlap, Etched Alum/Etched Alum
 1900 psi
@Temperature 83.0 °C
Overlap, Etched Alum/Etched Alum
 3100 psi
@Temperature -55.0 °C
Overlap, Etched Alum/Etched Alum
 3150 psi
@Temperature 23.0 °C
Overlap, Etched Alum/Etched Alum
Peel Strength 9.00 pli180° T-Peel, Black SBR/CRS
 11.0 pli180° T-Peel, Neoprene/CRS
 19.0 pli180° T-Peel, Etched Al/Etched Al
 22.0 pli180° T-Peel, Etched Al/Etched Al
 22.0 pli180° T-Peel, Etched Al/Etched Al
 22.0 pli180° T-Peel, Etched Al/Etched Al
 22.0 pli180° T-Peel, Etched Al/Etched Al
 22.0 pli180° T-Peel, Etched Al/Etched Al
 22.0 pli180° T-Peel, Nitrile/CRS
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.20e+12 ohm-cmASTM D257
Surface Resistance >= 1.60e+14 ohmASTM D257
Dielectric Constant 2.8
@Frequency 10000 Hz
ASTM D150
 2.8
@Frequency 100000 Hz
ASTM D150
 3.0
@Frequency 1000 Hz
ASTM D150
 3.1
@Frequency 500 Hz
ASTM D150
Dissipation Factor 0.022
@Frequency 100000 Hz
ASTM D150
 0.032
@Frequency 10000 Hz
ASTM D150
 0.065
@Frequency 1000 Hz
ASTM D150
 0.083
@Frequency 500 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µm/m-°C
@Temperature 20.0 - 70.0 °C
Glass Transition Temp, Tg 58.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 48.0 hourFull cure
 
Descriptive Properties
AppearanceOff-whiteBase
 Pale Yellow
 YellowAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Innospec FLEXAREN® 18001 EVA-Copolymer
DuPont Mobility and Materials Kalrez® 9500 Fluoroelastomer
Cookson Group STAYSTIK® 682 Aluminum Nitride Filled Thermally Enhanced Film
Arlon Electronic Materials 33N Polyimide Laminate and Prepreg
3M Scotch-Weld™ DP825 Acrylic Adhesives

PMM34595 / 169342

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.