MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cookson Group STAYSTIK® 682 Aluminum Nitride Filled Thermally Enhanced Film  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic

Material Notes: These thermoplastic adhesive films are designed for use in a variety of electronic applications. These materials are characterized by their excellent bonding. These films can be used for die attach and/or substrate attach in hybrid or Multi-Chip Modules (MCMs). The unique reworkability of this thermoplastic adhesive system offers many advantages in applications traditionally ill-suited to thermoset adhesives.

Features:

  • Fully polymerized resin - No "cure"
  • Easily reworkable - No outgassing
  • Bonds in seconds - Not hours or minutes
  • Low modulus reduces stress to bonded materials

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity >= 2.41 GPa>= 350 ksi
Adhesive Bond Strength >= 17.2 MPa>= 2500 psiDie shear adhesion, at 25°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+9 ohm-cm>= 1.00e+9 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity >= 1.00 W/m-K>= 6.94 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °FContinuous use
 <= 300 °C<= 572 °FExcursion Temperature
Minimum Service Temperature, Air -65.0 °C-85.0 °FContinuous use
Glass Transition Temp, Tg >= 98.0 °C>= 208 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Monthat 25°C
 
Descriptive Properties
Attach Temperature160-275°C
Filler MaterialAluminum Nitride

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Forged Plate
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Innospec FLEXAREN® 18001 EVA-Copolymer
Arlon Electronic Materials 33N Polyimide Laminate and Prepreg
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)

PPLASK042 / 56332

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.