MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Thermoplastic polyurethane elastomer for ink

Abrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applications.

Information provided by Taiwan Sheen Soon Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 - 1.20 g/cc0.0419 - 0.0434 lb/in³
Viscosity 20000 - 30000 cP20000 - 30000 cP30% solid in Anone/MEK
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 93 - 9793 - 97
Tensile Strength 44.1 MPa6400 psi
Elongation at Break 400 %400 %
100% Modulus 8.83 MPa
@Strain 100 %
1280 psi
@Strain 100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zhejiang Juner SAN-100 Second Injection Shot-Sticky TPE
Shandong Dawn Dawnprene 11-90A TPV (EPDM/PP)
Network Polymers Softflex® 9000
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy
Lubrizol ESTANE® T4086 Ester Based Thermoplastic Polyurethane

PSHEEN855 / 156259

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.