MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Network Polymers Softflex® 9000
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Softflex® Thermoplastic Elastomer Alloy

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0070 - 0.0080 cm/cm
@Thickness 3.17 mm
0.0070 - 0.0080 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 - 0.0080 cm/cm
@Thickness 3.17 mm
0.0070 - 0.0080 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow  3.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.4 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
 36 g/10 min
@Load 1.00 kg,
Temperature 235 °C
36 g/10 min
@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 87 - 9787 - 97Instantaneous; ASTM D2240
Hardness, Shore D 6565
Tensile Strength, Yield 44.8 MPa6500 psichs 20 in/min; ASTM D412
Elongation at Break 450 %450 %ASTM D412
50% Modulus 7.60 MPa
@Strain 50 %
7.60 MPa
@Strain 50 %
ASTM D412
100% Modulus 11.2 MPa
@Strain 100 %
1620 psi
@Strain 100 %
ASTM D412
300% Modulus 24.8 MPa
@Strain 300 %
3600 psi
@Strain 300 %
ASTM D412
Tear Strength 133 kN/m759 pli
Taber Abrasion, mg/1000 Cycles 1010H22 Wheel 1000 g load/1000 cycles; ASTM D3389
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B, at 25% deflection; ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chengdu Polyster 9500 General Grade TPV
Dow Engage® 8100 Polyolefin Elastomer
Dow Engage® Polyolefin Elastomer
Kuraray SEPTON® S2104 Thermoplastic Rubber
Zhejiang Juner SAN-100 Second Injection Shot-Sticky TPE

PDIAM026 / 29864

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.