MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Master Bond MasterSil 920-LO Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Key Features:
  • Meets NASA ASTM E595
  • Moderate viscosity with good flow properties
  • Excellent Neutral type cure
  • Superb optical clarity
Product Description: MasterSil 920-LO is a high performance, RTV silicone for sealing, coating and small encapsulations. First and foremost, it meets NASA low outgassing specifications. It is a neutral curing, non-corrosive type system. Also it has very good flow properties and outstanding electrical insulation values. These properties facilitate its use as a conformal coating and encapsulation system. With a softer durometer than many other silicones, it is particularly well suited for protecting sensitive electronic components. In fact, since it is low outgassing and optically clear, it can be used for select optical applications where delicate components must be protected. Similar to other one part silicones, the curing mechanism is based on humidity; the higher it is, the faster the cure. Also thinner sections cure more quickly than thicker ones. Another noteworthy property is its wide service temperature range of -175°F to +500°F. MasterSil 920-LO bonds very well to a wide variety of substrates including metals, glass as well as many plastics and rubber materials. With its inherent robust flexibility, the system can withstand the most rigorous kinds of thermal cycling and shock. MasterSil 920-LO is a “go-to material” in the encapsulation of sensitive electronic and optical components, especially when low outgassing and low stress are critical requirements. It should be noted, in order to achieve the low outgassing properties, a seven day cure at room temperature is recommended.

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
Viscosity 5000 - 10000 cP5000 - 10000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 25 - 3525 - 35
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 2.5
@Frequency 60 Hz
2.5
@Frequency 60 Hz
Dielectric Strength 19.7 kV/mm
@Thickness 3.17 mm
500 kV/in
@Thickness 0.125 in
Dissipation Factor 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -115 °C-175 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.431.43
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min168 hour
Tack-Free Time 45.0 - 60.0 min0.750 - 1.00 hour
Working Life 10.0 - 15.0 min10.0 - 15.0 min
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Master Bond MasterSil 155 Silicone
Master Bond Mastersil 713 Low Viscosity One Component Silicone
Master Bond MasterSil 921-LO Silicone

PMASTM940 / 185533

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.