MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond MasterSil 155 Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Key Features:
  • Superb electrical conductivity
  • User friendly handling
  • Cures to a tough, flexible black rubber
  • Withstands temperatures up to 400°F
Product Description: Master Bond MasterSil 155 is a two component black colored electrically conductive silicone compound for high performance bonding and sealing. The specifically modified graphite filled silicone resin after the addition of a liquid curing agent cures at ambient or more quickly at elevated temperatures to a tough, flexible, electrically conductive silicone rubber. The tightly controlled viscosity of this silicone elastomer formulation produces a smooth paste which assures complete fill-in around complicated contours in even very complex configurations and provides excellent electrical conductivity as well as superior resistance to vibration and shock after cure. It has been widely accepted for bonding and/or sealing of electronic components, electrical devices and various electro-optical systems as well for special electronic circuitry or wherever a tough, elastic electrically conductive adhesive, sealant or gasket offering superior protection against adverse environmental conditions is required. MasterSil 155 has a service temperature range of -85°F to +400°F.

Product Advantages:

  • Convenient mix ratio of base resin to curing agent: 1:1 by weight
  • Ready cure at ambient temperatures or faster cure at elevated temperatures
  • Excellent shock and vibration resistance
  • High tensile strength and elongation
  • Very low shrinkage upon cure-less of less than 0.15%
  • Superior electrical conductivity properties

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Linear Mold Shrinkage <= 0.0015 cm/cm<= 0.0015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength 4.83 - 5.52 MPa700 - 800 psi
Elongation at Break >= 300 %>= 300 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 20 - 40 ohm-cm20 - 40 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C4.44 µin/in-°F
Thermal Conductivity 1.15 - 1.59 W/m-K8.00 - 11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 149 °C
0.167 hour
@Temperature 300 °F
 30.0 min
@Temperature 107 °C
0.500 hour
@Temperature 225 °F
 120 - 240 min
@Temperature 65.6 °C
2.00 - 4.00 hour
@Temperature 150 °F
 8640 - 10100 min
@Temperature 23.9 °C
144 - 168 hour
@Temperature 75.0 °F
Working Life 480 min480 min100 g. batch; 8
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Colorblack
Mixing Ratio1:1 by weightPart A to B
ViscositypastePart A
 pastePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 151AO Thermally Conductive Silicone System
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Master Bond EP42HT-2LTE Two Component Epoxy
Master Bond Mastersil 705TC One Component, Thermally Conductive Silicone

PMASTM932 / 185525

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.