MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Description: Master Bond MB600S is a silver containing aqueous based sodium silicate system used as a coating in situations where EMI shielding effectiveness is paramount. Electromagnetic interference (EMI) and radio frequency interference (RFI) are very important issues in the world of electronics. The energy emitted from various sources such as radios, appliances, etc. can interfere with other electronic devices that are made from plastics. Conductive coatings are often applied to the housings in order to protect the devices from these types of interferences. One of the ways shielding effectiveness is measured is by attenuation. Technically, it refers to the differences of an incoming intensity of the source and its diminution after it passes through the coating. The actual unit of measurement is in decibels (dB). It should be noted that this scale is logarithmic and a difference of 10 dBs indicates ten times the shielding effectiveness (e.g. 40 dBs is ten times as effective as 30 dBs). In general, an effectiveness of 10-30 dBs is considered to be low, between 60-90 dBs is high and 90-120 dBs is exceptional. With the MB600S, the test method used was based on IEEE 299, 2006. Aluminum is considered the reference for this test, which was performed at room temperature. From 100 MHz to 2 GHz, the MB600S was as effective as the aluminum reference with a range of 95-105 dBs. Above 2 GHz the shielding effectiveness of MB600S decreased to the region around 80 dBs and slightly below. Above 4 GHz the effectiveness was in the 60-70 dB region. The performance of MB600S is truly fantastic. Aside from the stunning proficiency, the handling is wonderfully simple and safe. It is easy to brush on and being water based, the system is relatively non-toxic. It should be noted that it is possible to spray this system as well, with the proper equipment. If sprayed on, the shielding effectiveness would be even greater than the values given above. MB600S will cure at room temperature in 24-48 hours or in 1-2 hours at 80°C. If curing with heat it is advisable to ramp up the temperature over a 15-30 minute interval to prevent any possible blistering of the material. MB600S can be used in a wide variety of aerospace and electronic applications where superlative shielding effectiveness is desirable.

Key Features

  • Excellent shielding effectiveness
  • Silver conductive system
  • Temperature resistance up to +700°F
  • Easy application
Product Advantages:
  • Water based system, relatively non-toxic
  • Excellent temperature resistance
  • Excellent shielding effectiveness
  • Bonds well to a wide variety of substrates
  • Highly effective moisture barrier
  • Easily applied by brushing

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.40 g/cc4.40 g/cc
Solids Content 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohm
Shielding Effectiveness  60 - 80 dB
@Frequency 4.00e+9 - 1.80e+10 Hz
60 - 80 dB
@Frequency 4.00e+9 - 1.80e+10 Hz
 90 - 100 dB
@Frequency 2.00e+9 - 3.00e+9 Hz
90 - 100 dB
@Frequency 2.00e+9 - 3.00e+9 Hz
 100 - 105 dB
@Frequency 1.00e+9 - 2.00e+9 Hz
100 - 105 dB
@Frequency 1.00e+9 - 2.00e+9 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 371 °C700 °F
Minimum Service Temperature, Air -17.8 °C0.000 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature >=79.4 °C
1.00 - 2.00 hour
@Temperature >=175 °F
 1440 - 2880 min
@Temperature 23.9 °C
24.0 - 48.0 hour
@Temperature 75.0 °F
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond FL901AO One Component Thermally Conductive Epoxy Adhesive Film
Master Bond FL901S One Component, Silver Filled Epoxy
Master Bond FLM36 B-staged film for high performance bonding and sealing

PMASTB331 / 149578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.