MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.45 - 1.89 g/ccAverage value: 1.75 g/cc Grade Count:16
Filler Content 45.0 - 50.0 %Average value: 45.7 % Grade Count:7
Water Absorption 0.0100 - 0.100 %Average value: 0.0575 % Grade Count:4
Moisture Absorption at Equilibrium 0.00600 - 1.10 %Average value: 0.372 % Grade Count:3
Linear Mold Shrinkage 0.000 - 0.00200 cm/cmAverage value: 0.000861 cm/cm Grade Count:14
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cmAverage value: 0.00428 cm/cm Grade Count:14
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 58.0 - 93.0Average value: 76.8 Grade Count:4
Tensile Strength, Ultimate 88.0 - 180 MPaAverage value: 127 MPa Grade Count:16
 20.0 - 190 MPa
@Temperature -40.0 - 250 °C
Average value: 85.1 MPa Grade Count:3
 20.0 - 190 MPa
@Thickness 1.00 - 4.00 mm
Average value: 85.1 MPa Grade Count:3
Elongation at Break 0.600 - 3.30 %Average value: 1.37 % Grade Count:16
 0.300 - 0.900 %
@Temperature -40.0 - 250 °C
Average value: 0.633 % Grade Count:2
 0.300 - 0.900 %
@Thickness 1.00 - 4.00 mm
Average value: 0.633 % Grade Count:2
Modulus of Elasticity 12.0 - 24.5 GPaAverage value: 18.7 GPa Grade Count:14
 6.00 - 27.0 GPa
@Temperature -40.0 - 250 °C
Average value: 15.6 GPa Grade Count:3
 6.00 - 27.0 GPa
@Thickness 1.00 - 4.00 mm
Average value: 15.6 GPa Grade Count:3
Flexural Yield Strength 158 - 260 MPaAverage value: 196 MPa Grade Count:16
 10.0 - 300 MPa
@Temperature -40.0 - 250 °C
Average value: 121 MPa Grade Count:3
 10.0 - 300 MPa
@Thickness 0.790 - 4.00 mm
Average value: 121 MPa Grade Count:3
Flexural Modulus 10.0 - 24.0 GPaAverage value: 17.3 GPa Grade Count:16
 5.00 - 25.5 GPa
@Temperature -40.0 - 250 °C
Average value: 13.8 GPa Grade Count:3
 5.00 - 25.5 GPa
@Thickness 0.790 - 4.00 mm
Average value: 13.8 GPa Grade Count:3
Compressive Yield Strength 21.3 - 152 MPaAverage value: 88.4 MPa Grade Count:5
Compressive Modulus 18.0 - 21.0 GPaAverage value: 19.8 GPa Grade Count:3
Izod Impact, Notched 0.588 - 2.50 J/cmAverage value: 1.38 J/cm Grade Count:5
Izod Impact, Unnotched 3.16 - 6.53 J/cmAverage value: 4.80 J/cm Grade Count:4
Izod Impact, Notched (ISO) 8.00 - 16.0 kJ/m²Average value: 10.9 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.00 - 1.90 J/cm²Average value: 1.64 J/cm² Grade Count:8
 1.20 - 1.30 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 1.27 J/cm² Grade Count:4
Charpy Impact, Notched 0.360 - 1.20 J/cm²Average value: 0.905 J/cm² Grade Count:12
 0.800 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.950 J/cm² Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cmAverage value: 3.00e+15 ohm-cm Grade Count:12
Surface Resistance 1.00e+11 - 1.00e+17 ohmAverage value: 9.84e+15 ohm Grade Count:11
Dielectric Constant 3.40 - 5.00Average value: 4.32 Grade Count:13
 5.20 - 5.60
@Temperature 120 - 200 °C
Average value: 5.37 Grade Count:2
 5.20 - 5.60
@Frequency 60.0 - 1.00e+6 Hz
Average value: 5.37 Grade Count:2
Dielectric Strength 21.0 - 45.0 kV/mmAverage value: 31.0 kV/mm Grade Count:11
 20.0 - 40.0 kV/mm
@Temperature 100 - 200 °C
Average value: 27.6 kV/mm Grade Count:3
 20.0 - 40.0 kV/mm
@Thickness 0.800 - 3.20 mm
Average value: 27.6 kV/mm Grade Count:3
Dissipation Factor 0.00600 - 0.0310Average value: 0.0172 Grade Count:13
 0.00800 - 0.0830
@Temperature 120 - 200 °C
Average value: 0.0226 Grade Count:2
 0.00800 - 0.0830
@Frequency 60.0 - 1.00e+6 Hz
Average value: 0.0226 Grade Count:2
Arc Resistance 180 - 182 secAverage value: 181 sec Grade Count:3
Comparative Tracking Index 150 - 250 VAverage value: 192 V Grade Count:11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.00 - 15.0 µm/m-°CAverage value: 4.91 µm/m-°C Grade Count:12
 -1.00 - 7.00 µm/m-°C
@Temperature 55.0 - 260 °C
Average value: 2.88 µm/m-°C Grade Count:4
 -1.00 - 7.00 µm/m-°C
@Thickness 2.00 - 4.00 mm
Average value: 2.88 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 17.0 - 80.0 µm/m-°CAverage value: 55.1 µm/m-°C Grade Count:12
 76.0 - 100 µm/m-°C
@Temperature 55.0 - 260 °C
Average value: 83.8 µm/m-°C Grade Count:4
 76.0 - 100 µm/m-°C
@Thickness 2.00 - 4.00 mm
Average value: 83.8 µm/m-°C Grade Count:4
Specific Heat Capacity 1.50 J/g-°CAverage value: 1.50 J/g-°C Grade Count:3
Thermal Conductivity 0.320 - 0.400 W/m-KAverage value: 0.357 W/m-K Grade Count:3
Melting Point 280 - 357 °CAverage value: 338 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 240 - 315 °CAverage value: 285 °C Grade Count:16
Deflection Temperature at 8.0 MPa 203 - 271 °CAverage value: 233 °C Grade Count:3
UL RTI, Electrical 130 - 240 °CAverage value: 210 °C Grade Count:5
UL RTI, Mechanical with Impact 130 - 210 °CAverage value: 189 °C Grade Count:5
UL RTI, Mechanical without Impact 130 - 240 °CAverage value: 209 °C Grade Count:4
Flammability, UL94 V-0Grade Count:14
Oxygen Index 33.0 - 45.0 %Average value: 40.2 % Grade Count:5
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 370 °CAverage value: 143 °C Grade Count:7
Die Temperature 290 - 370 °CAverage value: 344 °C Grade Count:7
Melt Temperature 270 - 375 °CAverage value: 342 °C Grade Count:14
Mold Temperature 30.0 - 160 °CAverage value: 87.0 °C Grade Count:9
Drying Temperature 150 - 170 °CAverage value: 151 °C Grade Count:13
Moisture Content 0.0100 %Average value: 0.0100 % Grade Count:12
Injection Pressure 50.0 - 150 MPaAverage value: 100 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled

O2245 / 77948

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.