MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 - 1.81 g/cc0.0546 - 0.0654 lb/in³Average value: 1.71 g/cc Grade Count:47
 1.39 - 1.39 g/cc
@Temperature >=335 °C
0.0502 - 0.0502 lb/in³
@Temperature >=635 °F
Average value: 1.39 g/cc Grade Count:1
Filler Content 40.0 %40.0 %Average value: 40.0 % Grade Count:9
Water Absorption 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0350 % Grade Count:6
Moisture Absorption at Equilibrium 0.00200 - 0.0400 %0.00200 - 0.0400 %Average value: 0.0108 % Grade Count:10
Water Absorption at Saturation 0.00400 - 0.0700 %0.00400 - 0.0700 %Average value: 0.0247 % Grade Count:9
Linear Mold Shrinkage -0.000300 - 0.00400 cm/cm-0.000300 - 0.00400 in/inAverage value: 0.00118 cm/cm Grade Count:43
Linear Mold Shrinkage, Transverse 0.00200 - 0.0120 cm/cm0.00200 - 0.0120 in/inAverage value: 0.00560 cm/cm Grade Count:38
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 44.0 - 96.044.0 - 96.0Average value: 67.0 Grade Count:9
Hardness, Rockwell R 105105Average value: 105 Grade Count:3
Tensile Strength, Ultimate 3.00 - 177 MPa435 - 25700 psiAverage value: 127 MPa Grade Count:49
Elongation at Break 0.500 - 4.00 %0.500 - 4.00 %Average value: 1.94 % Grade Count:48
Modulus of Elasticity 7.50 - 34.5 GPa1090 - 5000 ksiAverage value: 14.7 GPa Grade Count:45
Flexural Yield Strength 109 - 250 MPa15800 - 36300 psiAverage value: 181 MPa Grade Count:49
Flexural Modulus 7.20 - 27.6 GPa1040 - 4000 ksiAverage value: 14.1 GPa Grade Count:49
Flexural Strain at Break 1.80 - 3.20 %1.80 - 3.20 %Average value: 2.45 % Grade Count:11
Compressive Yield Strength 53.0 - 134 MPa7690 - 19400 psiAverage value: 101 MPa Grade Count:7
Compressive Modulus 7.70 - 18.0 GPa1120 - 2610 ksiAverage value: 13.2 GPa Grade Count:7
Izod Impact, Notched 0.534 - 1.12 J/cm1.00 - 2.10 ft-lb/inAverage value: 0.804 J/cm Grade Count:9
Izod Impact, Unnotched 2.67 - 4.27 J/cm5.00 - 8.00 ft-lb/inAverage value: 3.38 J/cm Grade Count:3
Izod Impact, Notched (ISO) 3.50 - 60.0 kJ/m²1.67 - 28.6 ft-lb/in²Average value: 17.0 kJ/m² Grade Count:27
Izod Impact, Unnotched (ISO) 20.0 - 45.0 kJ/m²9.52 - 21.4 ft-lb/in²Average value: 26.3 kJ/m² Grade Count:6
 20.0 - 20.0 kJ/m²
@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 20.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 1.30 - 5.50 J/cm²6.19 - 26.2 ft-lb/in²Average value: 3.10 J/cm² Grade Count:19
 1.80 - 4.00 J/cm²
@Temperature -30.0 - -30.0 °C
8.57 - 19.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.45 J/cm² Grade Count:4
Charpy Impact, Notched 0.400 - 3.00 J/cm²1.90 - 14.3 ft-lb/in²Average value: 1.20 J/cm² Grade Count:31
 0.600 - 1.50 J/cm²
@Temperature -30.0 - -30.0 °C
2.86 - 7.14 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.27 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1e+05 - 1.00e+17 ohm-cm1e+05 - 1.00e+17 ohm-cmAverage value: 1.09e+16 ohm-cm Grade Count:25
Surface Resistance 1.00e+7 - 1.00e+17 ohm1.00e+7 - 1.00e+17 ohmAverage value: 2.12e+16 ohm Grade Count:26
Dielectric Constant 3.10 - 4.973.10 - 4.97Average value: 3.89 Grade Count:23
Dielectric Strength 18.0 - 59.0 kV/mm457 - 1500 kV/inAverage value: 36.0 kV/mm Grade Count:19
Dissipation Factor 0.00200 - 0.07000.00200 - 0.0700Average value: 0.0222 Grade Count:23
Arc Resistance 130 - 180 sec130 - 180 secAverage value: 156 sec Grade Count:6
Comparative Tracking Index 150 - 250 V150 - 250 VAverage value: 184 V Grade Count:24
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.00 - 25.0 µm/m-°C0.556 - 13.9 µin/in-°FAverage value: 6.15 µm/m-°C Grade Count:34
 -2.00 - 3.00 µm/m-°C
@Temperature 55.0 - 320 °C
-1.11 - 1.67 µin/in-°F
@Temperature 131 - 608 °F
Average value: 1.79 µm/m-°C Grade Count:2
 -2.00 - 5.00 µm/m-°C
@Temperature 55.0 - 320 °C
-1.11 - 2.78 µin/in-°F
@Temperature 131 - 608 °F
Average value: 1.79 µm/m-°C Grade Count:4
 -2.00 - 5.00 µm/m-°C
@Thickness 2.00 - 4.00 mm
-1.11 - 2.78 µin/in-°F
@Thickness 0.0787 - 0.157 in
Average value: 1.79 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 11.0 - 82.0 µm/m-°C6.11 - 45.6 µin/in-°FAverage value: 52.1 µm/m-°C Grade Count:31
 71.0 - 88.0 µm/m-°C
@Temperature 55.0 - 320 °C
39.4 - 48.9 µin/in-°F
@Temperature 131 - 608 °F
Average value: 84.1 µm/m-°C Grade Count:2
 71.0 - 94.0 µm/m-°C
@Temperature 55.0 - 320 °C
39.4 - 52.2 µin/in-°F
@Temperature 131 - 608 °F
Average value: 84.1 µm/m-°C Grade Count:4
 71.0 - 94.0 µm/m-°C
@Thickness 2.00 - 4.00 mm
39.4 - 52.2 µin/in-°F
@Thickness 0.0787 - 0.157 in
Average value: 84.1 µm/m-°C Grade Count:4
Melting Point 280 - 357 °C536 - 675 °FAverage value: 331 °C Grade Count:35
Deflection Temperature at 0.46 MPa (66 psi) 250 - 286 °C482 - 547 °FAverage value: 271 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 215 - 356 °C419 - 673 °FAverage value: 267 °C Grade Count:49
Deflection Temperature at 8.0 MPa 119 - 267 °C246 - 513 °FAverage value: 191 °C Grade Count:8
Vicat Softening Point 146 - 239 °C295 - 462 °FAverage value: 196 °C Grade Count:9
UL RTI, Electrical 130 - 240 °C266 - 464 °FAverage value: 191 °C Grade Count:5
UL RTI, Mechanical with Impact 130 - 220 °C266 - 428 °FAverage value: 180 °C Grade Count:5
UL RTI, Mechanical without Impact 130 - 240 °C266 - 464 °FAverage value: 199 °C Grade Count:4
Flammability, UL94 V-0V-0Grade Count:33
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 391 °C68.0 - 735 °FAverage value: 172 °C Grade Count:31
Die Temperature 290 - 380 °C554 - 716 °FAverage value: 342 °C Grade Count:25
Melt Temperature 270 - 385 °C518 - 725 °FAverage value: 336 °C Grade Count:40
Mold Temperature 30.0 - 150 °C86.0 - 302 °FAverage value: 89.6 °C Grade Count:17
Injection Velocity 150 mm/sec5.91 in/secAverage value: 150 mm/sec Grade Count:4
Drying Temperature 135 - 170 °C275 - 338 °FAverage value: 154 °C Grade Count:38
Moisture Content 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:35
Injection Pressure 34.5 - 150 MPa5000 - 21800 psiAverage value: 96.8 MPa Grade Count:29
Hot-Working Temperature 300 - 345 °C572 - 653 °FAverage value: 331 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

O2244 / 77947

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.