MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

VICTREX™ PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Product Description:

High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contact compliant, colour black.

Typical Application Areas:

Applications for higher strength and stiffness in a static or dynamic system. Excellent wear resistance, low coefficient of friction, low coefficient of thermal expansion. Chemically resistant to aggressive environments.

Information Provided by Victrex.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³Crystalline; ISO 1183
Water Absorption at Saturation  0.35 %
@Temperature 23.0 °C
0.35 %
@Temperature 73.4 °F
Equilibrium; by immersion; ISO 62-1
 0.50 %
@Temperature 100 °C
0.50 %
@Temperature 212 °F
immersion; ISO 62-1
Viscosity 525000 cP
@Temperature 400 °C
525000 cP
@Temperature 752 °F
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in395°C nozzle, 200°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in395°C nozzle, 200°C tool; ISO 294-4
Spiral Flow 10.0 cm
@Thickness 1.00 mm
3.94 in
@Thickness 0.0394 in
Mold Temp: 200°C, Melt Temp: 395°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 86
@Temperature 23.0 °C
86
@Temperature 73.4 °F
ISO 868
Tensile Strength at Break 230 MPa
@Temperature 23.0 °C
33400 psi
@Temperature 73.4 °F
ISO 527
Elongation at Break 2.1 %
@Temperature 23.0 °C
2.1 %
@Temperature 73.4 °F
ISO 527
Tensile Modulus 19.5 GPa
@Temperature 23.0 °C
2830 ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength 340 MPa
@Temperature 23.0 °C
49300 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 16.5 GPa
@Temperature 23.0 °C
2390 ksi
@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 9.50 kJ/m²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180/U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cm1V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  8.00 µm/m-°C
@Temperature <=143 °C
4.44 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 8.00 µm/m-°C
@Temperature >=143 °C
4.44 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
CTE, linear, Transverse to Flow  45.0 µm/m-°C
@Temperature <=143 °C
25.0 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 110 µm/m-°C
@Temperature >=143 °C
61.1 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
Melting Point 343 °C649 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 325 °C617 °FISO 75-f
Glass Transition Temp, Tg 143 °C289 °FOnset; ISO 11357
 150 °C302 °FMidpoint; ISO 11357
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 100 °C<= 212 °FHopper Temperature
Rear Barrel Temperature 375 °C707 °F
Middle Barrel Temperature 380 - 385 °C716 - 725 °F
Front Barrel Temperature 390 °C734 °F
Nozzle Temperature 395 °C743 °F
Mold Temperature 180 - 210 °C356 - 410 °F
Drying Temperature 120 - 150 °C
@Time 10800 - 18000 sec
248 - 302 °F
@Time 3.00 - 5.00 hour
 
Descriptive Properties
Gate>2 mm or 0.5 x part thickness
Runner>3.5mmmanifold
 >3mm Die/nozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
VICTREX™ PEEK 150GL30 30% Glass Fiber Reinforced
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
VICTREX™ PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced

PVICTA77 / 99755

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.