MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolan® 6403 Polystyrene, Extrusion
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Bapolan PS6403 is a high impact polystyrene resin designed for extrusion-thermoforming applications. It complies with US FDA21 CFR177.1640 and has a 94HB UL rating.

Application: General Purpose; Household Goods; Housings.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.

Key Words: General Purpose; High Gloss; High Impact Resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.0 g/10 min3.0 g/10 min200'C/5,000g; ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.5 MPa3550 psiASTM D-638
Elongation at Yield 46 %46 %ASTM D-638
Flexural Modulus, 1% Secant 2206 MPa320000 psiASTM D-790A
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/in@23'C; ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.5 °C200 °FASTM D-648
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processThermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Molded, Unreinforced
Overview of materials for Polystyrene, Extrusion Grade
Aclo Accucomp Polystyrene HS0600L High Impact
Bamberger Polymers Bapolan® 6450 Polystyrene Injection Molding Resin
Bamberger Polymers Bapolan® 6050 Polystyrene, Injection Grade

PBP3B310 / 20827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.