MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolan® 6450 Polystyrene Injection Molding Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Bapolan 6450 is a high impact polystyrene resin designed for injection molding applications requiring fast cycle times, superior impact and gloss. It complies with US FDA21 CFR177.1640 and has a 94HB UL rating.

Applications: General Purpose; Household Goods; Housings.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers. All data is based on molded plaques.

Key Words: Fast Molding Cycle; General Purpose; High Gloss; High Impact Resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.1 MPa3500 psiASTM D-638
Elongation at Yield 43 %43 %ASTM D-638
Flexural Modulus, 1% Secant 2240 MPa325000 psiASTM D-790A
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D-648
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolan® 6055 Polystyrene, Injection Molding
Bamberger Polymers Bapolan® 6050 Polystyrene, Injection Grade
Bamberger Polymers Bapolan® 6403 Polystyrene, Extrusion
Aclo Accucomp Polystyrene HS0600L High Impact
Overview of materials for Polystyrene, Molded, Unreinforced

PBP3B32E / 20830

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.