MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as well as thermal shock protection.

Emerson & Cuming 2651-40/23LV Stycast® Two-Component General Purpose Encapsulant
  • Good Chemical Resistance
  • Filled
  • Low viscosity
  • Thermally conductive
  • Mix Ratio by Weight = 100:18
Cure Type: Room Temp or Heat Bonding Type: Epoxy

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Viscosity 2200 cP
@Temperature 25.0 °C
2200 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dielectric Strength 17.7 kV/mm450 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 61.0 µm/m-°C
@Temperature 20.0 °C
33.9 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.550 W/m-K3.82 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 240 min2.00 - 4.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® 3861 Thermally Conductive Potting
Henkel Loctite® 3860 Thermally Conductive Potting
Trelleborg Emerson & Cuming Stycast® 1265 Two-Component Easy Mix Ratio Encapsulant
Trelleborg Emerson & Cuming Stycast® 2651-40FR/9 Two-Component Epoxy Flame Retardant Encapsulant
Overview of materials for Epoxy Encapsulant, Unreinforced

PEMERS42 / 35734

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.