Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as well as thermal shock protection.
Emerson & Cuming 2651-40/23LV Stycast® Two-Component General Purpose Encapsulant
- Good Chemical Resistance
- Filled
- Low viscosity
- Thermally conductive
- Mix Ratio by Weight = 100:18
Cure Type: Room Temp or Heat Bonding Type: Epoxy The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |