MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Trelleborg Emerson & Cuming Stycast® 2651-40FR/9 Two-Component Epoxy Flame Retardant Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes:
Features and Typical Applications
Provide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conductivity. Typical applications include a wide range of electrical components such as capacitors and transformers.

Emerson & Cuming 2651-40FR/9 Stycast® Two-Component Epoxy Flame Retardant Encapsulant
  • Thermally Conductive
  • Good Chemical Resistance
  • Filled
  • Mix Ratio by Weight = 100:9
Cure Type: Room Temp or Heat Bonding Type: Epoxy

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³
Viscosity 8000 cP8000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dielectric Strength 17.7 kV/mm450 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.550 W/m-K3.82 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 56.0 °C133 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 - 60.0 min0.500 - 1.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 1265 Two-Component Easy Mix Ratio Encapsulant
Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant
Henkel Loctite® 3861 Thermally Conductive Potting
Henkel Loctite® 3860 Thermally Conductive Potting
Trelleborg Emerson & Cuming Stycast® 1365-65 Two-Component Epoxy Flexible Encapsulant

PEMERS20 / 35712

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.