MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta RT630 Phenolic Paper Laminate Tube, NEMA XXX
Categories: Polymer; Thermoset; Phenolic

Material Notes: RT630 is a fine machining grade with excellent electrical properties and moisture resistance. It has good dimensional stability and resists splitting. Typical applications include fuse tubes, coil forms and supports. RT630 also complies with MIL-I-24768/10, Type PBE and ASTM D709 Type I Grade XXX.

Information provided by Norplex-Micarta

Key Words: Paper, Phenolic, Micarta, NEMA XXX, MIL-I-24768/10 Type PBE, ASTM D709 Type I Grade XXX
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/cc0.750" X 1.000"; ASTM D792
Moisture Absorption 0.800 %0.750" X 1.000"; ASTM D570 Condition D1-24/23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 1000.750" X 1.000"; ASTM D785
Tensile Strength 13500 psi0.750" X 1.000"; ASTM D638 Condition A
Compressive Strength 23500 psi0.750" X 1.000"; ASTM D695 Condition A
Compressive Modulus 415 ksi0.750" X 1.000"; ASTM D695 Condition A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.28
@Frequency 1e+6 Hz
0.750" X 1.000"; ASTM D150 Condition A
Dielectric Strength 265 V/mil0.750" X 1.000"; ASTM D149 Condition D-48/50
 450 V/mil0.750" X 1.000"; ASTM D149 Condition A
Dielectric Breakdown 23000 V0.750" X 1.000"; ASTM D149 Condition D-48/50
 60000 V0.750" X 1.000"; ASTM D149 Condition A
Dissipation Factor 0.013
@Frequency 1e+6 Hz
0.750" X 1.000"; ASTM D150 Condition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 140 °C0.750" X 1.000"; UL Bulletin 746b
UL RTI, Mechanical with Impact 130 °C0.750" X 1.000"; UL Bulletin 746b
Flammability, UL94 HB0.750" X 1.000"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta NP610 Phenolic Paper Laminate Sheet, NEMA X
Norplex-Micarta RT630H Phenolic Paper Laminate Tube, NEMA XXX
Norplex-Micarta RT628H Phenolic Paper Laminate Tube, NEMA XX
Norplex-Micarta RT628 Phenolic Paper Laminate Tube, NEMA XX
Norplex-Micarta RT630S Phenolic Paper Laminate Tube, NEMA XXX

PNORPM104 / 192843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.