MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP610 Phenolic Paper Laminate Sheet, NEMA X
Categories: Polymer; Thermoset; Phenolic

Material Notes: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.

Information provided by Norplex-Micarta

Key Words: Paper, Phenolic, Micarta, NEMA X, MIL-I-24768/12 - PBM, ASTM D709 Type I Grade X
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc
@Thickness 12.7 mm
1.40 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 1.80 %
@Thickness 1.57 mm
1.80 %
@Thickness 0.0620 in
ASTM D570 Condition D1-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 90
@Thickness 6.35 mm
90
@Thickness 0.250 in
ASTM D785
Tensile Strength  89.6 MPa
@Thickness 3.17 mm
13000 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 117 MPa
@Thickness 3.17 mm
17000 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  193 MPa
@Thickness 1.57 mm
28000 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 234 MPa
@Thickness 1.57 mm
34000 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Flexural Modulus  9.65 GPa
@Thickness 1.57 mm
1400 ksi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 13.1 GPa
@Thickness 1.57 mm
1900 ksi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Compressive Strength 241 MPa
@Thickness 12.7 mm
35000 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Shear Strength 103 MPa
@Thickness 1.57 mm
15000 psi
@Thickness 0.0620 in
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched  0.406 J/cm
@Thickness 12.7 mm
0.760 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 0.438 J/cm
@Thickness 12.7 mm
0.820 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 23.6 kV/mm
@Thickness 1.57 mm
600 kV/in
@Thickness 0.0620 in
ASTM D149 Condition A
Dielectric Breakdown 40000 V
@Thickness 1.57 mm
40000 V
@Thickness 0.0620 in
ASTM D149 Condition A
Arc Resistance 90 sec
@Thickness 3.17 mm
90 sec
@Thickness 0.125 in
ASTM D495 Conition A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Thickness 3.17 mm
7.22 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 17.0 µm/m-°C
@Thickness 3.17 mm
9.44 µin/in-°F
@Thickness 0.125 in
IPC-TM 650-2.4.24
UL RTI, Electrical 130 °C266 °FUL Bulletin 746b
UL RTI, Mechanical with Impact 130 °C266 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
 
Descriptive Properties
Bonding Strength1000[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta RT630H Phenolic Paper Laminate Tube, NEMA XXX
Norplex-Micarta NP629 Phenolic Paper Laminate Sheet, NEMA XX
Norplex-Micarta RT628H Phenolic Paper Laminate Tube, NEMA XX
Norplex-Micarta RT628 Phenolic Paper Laminate Tube, NEMA XX
Norplex-Micarta RT630 Phenolic Paper Laminate Tube, NEMA XXX

PNORPM004 / 192761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.