Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Information provided by Norplex-Micarta |
Paper, Phenolic, Micarta, NEMA X, MIL-I-24768/12 - PBM, ASTM D709 Type I Grade X |