MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta RT628H Phenolic Paper Laminate Tube, NEMA XX
Categories: Polymer; Thermoset; Phenolic

Material Notes: Being a heat treated version of RT628, RT628H is an improved machining grade meeting NEMA XX for tubes. It has low moisture absorption and good dimensional stability. Typical applications are as a replacement for RT629 where improved machining characteristics are needed. The primary application is in transformers.

Information provided by Norplex-Micarta

Key Words: Paper, Phenolic, Micarta, NEMA XX, MIL-I-24768/11 Type PBG, ASTM D709 Type I Grade XX
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/cc0.750" X 1.000"; ASTM D792
Moisture Absorption 1.30 %1.30 %0.750" X 1.000"; ASTM D570 Condition D1-24/23
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 85850.750" X 1.000"; ASTM D785
Compressive Strength 131 MPa19000 psi0.750" X 1.000"; ASTM D695 Condition A
Compressive Modulus 2.48 GPa360 ksi0.750" X 1.000"; ASTM D695 Condition A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.0 kV/mm330 kV/in0.750" X 1.000"; ASTM D149 Condition D-48/50
 14.2 kV/mm360 kV/in0.750" X 1.000"; ASTM D149 Condition A
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 130 °C266 °F0.750" X 1.000"; UL Bulletin 746b
UL RTI, Mechanical with Impact 130 °C266 °F0.750" X 1.000"; UL Bulletin 746b
Flammability, UL94 HBHB0.750" X 1.000"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta NP610 Phenolic Paper Laminate Sheet, NEMA X
Norplex-Micarta RT630H Phenolic Paper Laminate Tube, NEMA XXX
Norplex-Micarta NP629 Phenolic Paper Laminate Sheet, NEMA XX
Norplex-Micarta RT629 Phenolic Paper Laminate Tube, NEMA XX
Norplex-Micarta RT628 Phenolic Paper Laminate Tube, NEMA XX

PNORPM102 / 192841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.