MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Dow TC-5022 Thermally Conductive Compound
Categories: Fluid; Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.23 g/cc
@Temperature 25.0 °C
3.23 g/cc
@Temperature 77.0 °F
Viscosity 91000 cP91000 cPDynamic
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.50e+10 ohm-cm5.50e+10 ohm-cm
Dielectric Strength 4.53 kV/mm115 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 4.00 W/m-K27.8 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorGrey
FlowableYes
HydrophobicYes
Self LevelingYes
Water ResistantYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
5022 Aluminum Composition Spec
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O

PDOWCO811 / 106512

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.