MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chlorides and resistance to oxidation at elevated temperatures. An addition of 0.5% copper adds to corrosion resistance. Columbium (niobium) in the amount of about 0.5% is added for elevated temperature strength and also provides resistance to intergranular corrosion.

The AL 433 alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Fine columbium carbides may be visible in the ferrite matrix microstructure.

The AL 433 alloy can be machined, welded and formed like other stabilized, ferritic stainless steels. AL 433 alloy is an excellent candidate for elevated temperature applications where strength, combined with fabricability are needed.

Information provided by Allegheny Ludlum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7979typical
Tensile Strength, Ultimate  286 MPa
@Temperature 649 °C
41500 psi
@Temperature 1200 °F
typical
 401 MPa
@Temperature 204 °C
58200 psi
@Temperature 400 °F
typical
 492 MPa
@Temperature 23.0 °C
71400 psi
@Temperature 73.4 °F
Tensile Strength, Yield  286 MPa
@Temperature 649 °C
41500 psi
@Temperature 1200 °F
typical
 324 MPa
@Temperature 23.0 °C
47000 psi
@Temperature 73.4 °F
 401 MPa
@Temperature 204 °C
58200 psi
@Temperature 400 °F
typical
Elongation at Break 32 %32 %typical in 2" (50 mm)
Modulus of Elasticity 200 GPa29000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.44 µm/m-°C
@Temperature 20.0 - 100 °C
5.800 µin/in-°F
@Temperature 68.0 - 212 °F
 10.8 µm/m-°C
@Temperature 20.0 - 260 °C
6.00 µin/in-°F
@Temperature 68.0 - 500 °F
 11.25 µm/m-°C
@Temperature 20.0 - 480 °C
6.250 µin/in-°F
@Temperature 68.0 - 896 °F
 11.7 µm/m-°C
@Temperature 20.0 - 650 °C
6.50 µin/in-°F
@Temperature 68.0 - 1200 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 20.93 W/m-K145.3 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 %0.010 %
Chromium, Cr 20 %20 %
Copper, Cu 0.50 %0.50 %
Iron, Fe 78 %78 %as balance
Manganese, Mn 0.30 %0.30 %
Nickel, Ni 0.25 %0.25 %
Niobium, Nb (Columbium, Cb) <= 0.80 %<= 0.80 %
Nitrogen, N 0.019 %0.019 %
Phosphorus, P 0.021 %0.021 %
Silicon, Si 0.39 %0.39 %
Sulfur, S 0.0010 %0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum AL 418™ Special (Greek Ascoloy) Martensitic Stainless Steel
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Annealed
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper

NL433 / 17934

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.