Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
368
materials in the category
T 400 Series Stainless Steel
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
368
Results
-- Page
1
2
3
4
5
6
7
8
of
8
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for T 400 Series Stainless Steel
2
403 Stainless Steel, annealed, sheet
3
403 Stainless Steel, annealed, strip
4
403 Stainless Steel, soft tempered, wire 6.4 mm diameter
5
403 Stainless Steel, annealed, bar
6
403 Stainless Steel, tempered, bar
7
405 Stainless Steel, annealed, sheet
8
405 Stainless Steel, soft tempered wire, 6.4 mm diameter
9
405 Stainless Steel, annealed, plate
10
405 Stainless Steel, annealed, bar
11
405 Stainless Steel, annealed and cold drawn, 25 mm diameter
12
405 Stainless Steel
13
406 Stainless Steel
14
409 Stainless Steel, annealed sheet, strip, plate, bar
15
409 Stainless Steel
16
410 Stainless Steel
17
410 Stainless Steel, tempered at 233°C
18
410 Stainless Steel, tempered at 343°C
19
410 Stainless Steel, tempered at 453°C
20
410 Stainless Steel, tempered at 508°C
21
410 Stainless Steel, tempered at 568°C
22
410 Stainless Steel, tempered at 623°C
23
410 Stainless Steel, tempered at 678°C
24
410 Stainless Steel, tempered at 733°C
25
410 Stainless Steel, tempered at 650°C
26
410 Stainless Steel, tempered at 540°C (1000°F)
27
410 Stainless Steel, tempered at 605°C
28
AISI Type 410S Stainless Steel
29
AISI Type 410S Stainless Steel, tempered at 233°C
30
AISI Type 410S Stainless Steel, tempered at 343°C
31
AISI Type 410S Stainless Steel, tempered at 453°C
32
AISI Type 410S Stainless Steel, tempered at 508°C
33
AISI Type 410S Stainless Steel, tempered at 568°C
34
AISI Type 410S Stainless Steel, tempered at 623°C
35
AISI Type 410S Stainless Steel, tempered at 678°C
36
AISI Type 410S Stainless Steel, tempered at 733°C
37
AISI Type 410S Stainless Steel, tempered at 650°C
38
AISI Type 410S Stainless Steel, tempered at 540°C (1000°F)
39
AISI Type 410S Stainless Steel, tempered at 605°C
40
410 Cb Martensitic Stainless Steel (UNS S41040)
41
Type 410S Martensitic Stainless Steel, Annealed Forgings, UNS S41008
42
Type 410S Martensitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S41008
43
414 Stainless Steel
44
414 Stainless Steel, tempered at 233°C
45
414 Stainless Steel, tempered at 343°C
46
414 Stainless Steel, tempered at 453°C
47
414 Stainless Steel, tempered at 508°C
48
414 Stainless Steel, tempered at 568°C
49
414 Stainless Steel, tempered at 623°C
50
414 Stainless Steel, tempered at 678°C
Found
368
Results
-- Page
1
2
3
4
5
6
7
8
of
8
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.