System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Categories:
Polymer
;
Thermoset
;
Bismaleimide (BMI)
Material Notes:
Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% Voids
Information provided by HexCel
Key Words:
BMI
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Flexural Yield Strength
655
MPa
@Temperature 232 °C
Control (Prepreg with no freezer or out time exposure)
710
MPa
@Temperature 232 °C
Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
731
MPa
@Temperature 232 °C
Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
758
MPa
@Temperature 232 °C
Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
814
MPa
@Temperature 232 °C
Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
827
MPa
@Temperature 232 °C
Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
862
MPa
@Temperature 23.0 °C
869
MPa
@Temperature 23.0 °C
876
MPa
@Temperature 23.0 °C
889
MPa
@Temperature 23.0 °C
903
MPa
@Temperature 23.0 °C
924
MPa
@Temperature 23.0 °C
Compressive Yield Strength
469
MPa
@Temperature 232 °C
Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
474
MPa
@Temperature 232 °C
Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
481
MPa
@Temperature 232 °C
Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
499
MPa
@Temperature 232 °C
Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
532
MPa
@Temperature 232 °C
Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
558
MPa
@Temperature 232 °C
Control (Prepreg with no freezer or out time exposure)
606
MPa
@Temperature 23.0 °C
623
MPa
@Temperature 23.0 °C
703
MPa
@Temperature 23.0 °C
710
MPa
@Temperature 23.0 °C
731
MPa
@Temperature 23.0 °C
738
MPa
@Temperature 23.0 °C
Shear Strength
44.3
MPa
@Temperature 232 °C
Short Beam; Phase II (Prepreg stored in freezer 4 months at -9°C and exposed to 60 days at RT)
45.9
MPa
@Temperature 232 °C
Short Beam; Phase IV (Prepreg stored in freezer 1 year at -9°C and exposed to 30 days at RT)
46.1
MPa
@Temperature 232 °C
Short Beam; Phase I (Prepreg stored in freezer 4 months at -9°C and exposed to 30 days at RT)
47.2
MPa
@Temperature 232 °C
Short Beam; Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
49.6
MPa
@Temperature 23.0 °C
51.1
MPa
@Temperature 232 °C
Short Beam; Phase III (Prepreg stored in freezer 6 months at -9°C and exposed to 60 days at RT)
51.7
MPa
@Temperature 232 °C
Short Beam; Control (Prepreg with no freezer or out time exposure)
55.2
MPa
@Temperature 23.0 °C
56.5
MPa
@Temperature 23.0 °C
60.7
MPa
@Temperature 23.0 °C
64.1
MPa
@Temperature 23.0 °C
68.7
MPa
@Temperature 23.0 °C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive
Henkel Hysol EA 9673 (BMI) Film Adhesive
Evonik Compimide® TM124-ether 2,2'-Bis(4-allyloxyphenyl)propane
Evonik Compimide® TM124 2,2'-Bis(3-allyl-4-hydroxyphenyl)propane
PHEXC006 / 98476
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.