MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Compimide® TM124 2,2'-Bis(3-allyl-4-hydroxyphenyl)propane
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Compimide® TM124 (2,2'-Bis(3-allyl-4-hydroxyphenyl)propane, also known as o,o'-diallylbisphenol A, CAS 1745-89-7) is a co-monomer designed as a toughening modifier for the use with bismaleimide building blocks or with bismaleimide formulated resins to form tough and temperature resistant polymer networks. When formulated with bismaleimides, Compimide® TM124 provides thermosets with high glass transition temperatures. For instance, cured formulations with Compimide® buildings blocks and/or resins show Tg in the range of 275–285°C.

Key Words: BMI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 15 - 20 cP
@Temperature 25.0 °C
15 - 20 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 275 - 285 °C527 - 545 °F
 
Descriptive Properties
Purity>85%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Compimide® MDAB 4,4'-bismaleimidodiphenylmethane
Evonik Compimide® 353A Bismaleimide
Evonik Compimide® TM124-ether 2,2'-Bis(4-allyloxyphenyl)propane
Evonik Compimide® 1206R55 Bismaleimide
Evonik Compimide® TM123 4,4'-Bis(o-propenylphenoxy)benzophenone

PEVONIK04 / 120434

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.