MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Primary Processing Method: Injection Molding

Key Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation sterilization, easily processed

Applications: medical devices, syringes, test tubes, blood vials

Passed USP Class VI testing. All ingredients meet TSCA (US) and DSL (Canada).

Description: Pro-fax PF511 polypropylene homopolymer resin is designed for thermoformed container applications that require see-through clarity and good stiffness. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792B
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7474ASTM D785A
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Yield 16 %16 %ASTM D638
Flexural Modulus, 1% Secant 780 MPa113000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 0.330 J/cm0.618 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C169 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant
Sunoco D040A Homopolymer Polypropylene
LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified
ExxonMobil Exceed™ PP9074MED Polypropylene Homopolymer

PMO111 / 53526

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.