MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Primary Processing Method: Injection Molding and Injection Stretch Blow Molding

Key Features: clarified polypropylene random copolymer resin, superior clarity, good impact and rigidity balance, good surface finish and color, low odor and low taste transfer, improved injection molding cycle times

Applications: containers, housewares, bottles

Meets FDA requirements in 21 CFR 177.1520 for all food contact applications up to 212°F (100°C).

Description: Pro-fax SR549M clarified polypropylene random copolymer resin has good see-through and contact clarity in injection molding and injection stretch blow molding applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792B
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus, 1% Secant 1000 MPa145000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 0.660 J/cm1.24 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C183 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003A
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 7622MZ Polypropylene, Injection Molding Grade
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer

PMO168 / 53545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.