MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exceed™ PP9074MED Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.

Availability: Europe and North America

Features:

  • Controlled Rheology
  • E-beam Sterilizable
  • Ethylene Oxide Sterilizable
  • High Clarity
  • Radiation (Gamma) Resistant
  • Radiation Sterilizable
Uses:
  • Hypodermic Syringe Parts
  • Labware
  • Medical Packaging
  • Medical/Healthcare Applications
Processing Method: Injection Molding

Information provided by ExxonMobil

Key Words: ExxonMobil ™ PP9074MED
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
24 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2500 psi20 in/min; ASTM D638
Tensile Strength, Yield 32.8 MPa4750 psi20 in/min; ASTM D638
Elongation at Break 51 %51 %20 in/min; ASTM D638
Elongation at Yield 13 %13 %20 in/min; ASTM D638
Flexural Modulus, 1% Secant 1050 MPa153000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D256A
Gardner Impact 23.6 J
@Thickness 3.17 mm,
Temperature -28.9 °C
17.4 ft-lb
@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 8.6 %8.6 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills P5M6K-080 Polypropylene Random Copolymer
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant
ExxonMobil Exceed™ PP9122 Polypropylene Homopolymer
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
ExxonMobil PP1013H1 Polypropylene Homopolymer

PEX99414 / 175650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.