RT629 is a paper phenolic tube intended primarily for mechanical applications, but is suitable for electrical applications as well. The electrical properties are not quite as good as those of RT630. RT629 also complies with MIL-I-24768/11, Type PBG and ASTM D709 Type I Grade XX.Information provided by Norplex-Micarta |
Paper, Phenolic, Micarta, NEMA XX, MIL-I-24768/11 Type PBG, ASTM D709 Type I Grade XX |