MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 3R66 Seamless tube and pipe
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic stainless steel, ASTM type 316L

Sandvik 3R66 is a molybdenum-alloyed austenitic chromium-nickel steel. It is characterized by low contents of the interstitial elements carbon and nitrogen. The grade is specially developed for electronic tubing used in the production of micro-chips. Other applications are found in the food and drink as well as pharmaceutical industries where a very clean steel is required.

Information provided by Sandvik

ASTM 316L, MT316L; UNS S31603; EN 1.4435

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 155
Tensile Strength, Ultimate 515 - 690 MPa
 >= 360 MPa
@Temperature 600 °C
 >= 410 MPa
@Temperature 300 °C
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
 >= 250 MPa
@Strain 1 %
 >= 110 MPa
@Strain 0.2 %,
Temperature 600 °C
 >= 135 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 135 MPa
@Strain 1 %,
Temperature 600 °C
 >= 160 MPa
@Strain 1 %,
Temperature 300 °C
Elongation at Break >= 45 %
Modulus of Elasticity 200 GPa
 165 GPa
@Temperature 500 °C
 179 GPa
@Temperature 300 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
 17.0 µm/m-°C
@Temperature 30.0 - 200 °C
 18.0 µm/m-°C
@Temperature 30.0 - 500 °C
 18.5 µm/m-°C
@Temperature 30.0 - 700 °C
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
 0.515 J/g-°C
@Temperature 200 °C
 0.540 J/g-°C
@Temperature 400 °C
 0.575 J/g-°C
@Temperature 600 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 17.0 W/m-K
@Temperature 200 °C
 20.0 W/m-K
@Temperature 400 °C
 23.0 W/m-K
@Temperature 600 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 17.5 %
Iron, Fe 63.5 %As Balance
Manganese, Mn 1.7 %
Molybdenum, Mo 2.6 %
Nickel, Ni 14 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.60 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 316L Stainless Steel, annealed strip
AISI Type 316L Stainless Steel, annealed sheet
LG Chemical 402 AF Flame Retardant HIPS
Polynt DISTITRON® 514 CV2 Unsaturated Polyester Resin
HP Alloys Nitronic® 50 Austenitic Stainless, Annealed

NSANDV237 / 19131

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.