MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt DISTITRON® 514 CV2 Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Orthophthalic

Appearance: Neutral - Transparent

Main resin characteristics: Clear, unaccelerated

Main applications: Abrasives, chips

Molding information: Casting

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
Solids Content 56 - 60 %56 - 60 %MT-CU001C
Brookfield Viscosity 180 - 250 cP180 - 250 cPsp 2 rpm 20; MT-CU025V
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4545ASTM D 2583
Tensile Strength 70.0 MPa10200 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 4.00 GPa580 ksiISO 527
Flexural Strength 140 MPa20300 psiISO 178
Flexural Modulus 4.00 GPa580 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75 -2A
Glass Transition Temp, Tg 80.0 °C176 °FASTM E 1545
 
Processing PropertiesMetricEnglishComments
Cure Time 6.00 - 9.50 min
@Temperature 20.0 °C
0.100 - 0.158 hour
@Temperature 68.0 °F
Reactivity at 20°C + 0,9% Co 1% + 2% MEKP50; RS.08.G
Gel Time 7.00 - 9.00 min
@Temperature 20.0 °C
7.00 - 9.00 min
@Temperature 68.0 °F
Reactivity at 20°C + 0,9% Co 1% + 2% MEKP50; RS.08.G
Shelf Life 3.00 Month3.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm175 - 205°CRS.08.G; Reactivity at 20°C + 0,9% Co 1% + 2% MEKP50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical 402 AF Flame Retardant HIPS
Sandvik 3R66 Seamless tube and pipe
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade
A. Schulman Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2

PPOLYN9418 / 232013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.