MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Garlock 2930 Compressed Aramid Fiber Gasketing, Neoprene Binder
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Aramid fibers with a Neoprene binder.
  • Ideal for utility services
  • Excellent sealability
  • Improved thermal stability
  • Good for general service
Media: Water, steam, refrigerants, oils, fuels, mild acids, and mild alkalies

Information provided by Garlock Rubber Technologies

Key Words: chloroprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0608 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.8 MPa2000 psiacross grain; ASTM F152
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 371 °C700 °F
 204 °C
@Pressure 6.89 MPa
400 °F
@Pressure 1000 psi
Continuous
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorBlack
Compressibility, %7-17ASTM F36
Creep Relaxation, %22.5ASTM F38
Sealability ASTM F37B, ml/hr1ASTM Fuel A
 2Nitrogen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene
Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Polychloroprene Rubber (CR)

PGARL803 / 157483

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.