MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Aramid fiber, high-temperature fillers, and neoprene (CR) binder. Handles service conditions with refrigerants and various petroleum-based oils.
  • Excellent Sealability
  • Unique blend of aramid fibers, fillers, and a neoprene rubber binder provides improved torque retention and lowered emissions levels
Media: Water, Saturated Steam, Refrigerants, Oils, Fuels

Information provided by Garlock Rubber Technologies

Key Words: chloroprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0579 lb/in³
Permeability 0.0800.080Gas Permeability, cc/min; DIN 3535 Part 4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.5 MPa2250 psiacross grain; ASTM F152
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  >= 10.6 kV/mm
@Temperature 121 °C,
Time 10800 sec
>= 269 kV/in
@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
 >= 15.4 kV/mm
@Temperature 121 °C,
Time 10800 sec
>= 392 kV/in
@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
 2.87 kV/mm
@Thickness 3.17 mm
73.0 kV/in
@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
 3.07 kV/mm
@Thickness 1.59 mm
78.0 kV/in
@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 371 °C700 °F
 204 °C
@Pressure 8.27 MPa
400 °F
@Pressure 1200 psi
Continuous
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorBlack
Compressibility, %7-17ASTM F36
Creep Relaxation, %18ASTM F38
Sealability ASTM F37B, ml/hr0.2ASTM Fuel A
 1Nitrogen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Seals Eastern 5861 Fluoro-silicone
Garlock 2930 Compressed Aramid Fiber Gasketing, Neoprene Binder

PGARL808 / 157488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.