MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasing acrylonitrile content leads to higher hardness, strength, abrasion resistance, heat resistance, and oil/fuel resistance and lower resilience and low temperature flexibility. NBR is generally damaged by ozone, chlorinated solvents, ketones, aldehydes, esters, and nitrogen-containing solvents.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Base Elastomer
 1.15 - 1.35 g/cc0.0415 - 0.0488 lb/in³Compounded
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 30 - 9530 - 95Depends on compounding
Tensile Strength, Ultimate 6.89 - 24.1 MPa1000 - 3500 psiReinforced
 0.896 MPa
@Temperature 204 °C
130 psi
@Temperature 400 °F
 4.83 MPa
@Temperature 121 °C
700 psi
@Temperature 250 °F
Elongation at Break 400 - 600 %400 - 600 %Reinforced
 20 %
@Temperature 204 °C
20 %
@Temperature 400 °F
 120 %
@Temperature 121 °C
120 %
@Temperature 250 °F
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
200 mm/min
Compression Set 5.0 %5.0 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear 702 µm/m-°C
@Temperature 20.0 °C
390 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Brittleness Temperature -51.1 °C-60.0 °F
Glass Transition Temp, Tg -38.0 °C-36.4 °FTypical of rubber with 18% ACN content
 -2.00 °C28.4 °FTypical of rubber with 50% ACN content

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hydrogenated Nitrile Rubber (HNBR)
Nitriflex N-612B NBR - Nitrile Rubber
Ethylene Propylene Rubber (EPM, EPDM)
ATG s.r.l. NBR Nitrile-Butadiene Rubber
Vicone High Performance Rubber VicoSeal™ 617N-BK Rubber Vulcanized to SS304

P0RU01 / 20051

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.