MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 612, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Impact Modified

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.820 - 1.11 g/ccAverage value: 1.02 g/cc Grade Count:17
Water Absorption 0.900 - 1.20 %Average value: 0.975 % Grade Count:8
Moisture Absorption at Equilibrium 0.650 - 1.00 %Average value: 0.775 % Grade Count:4
Water Absorption at Saturation 2.10 - 2.80 %Average value: 2.38 % Grade Count:8
Viscosity 150000 - 150000 cP
@Temperature 280 - 280 °C
Average value: 150000 cP Grade Count:1
 150000 - 150000 cP
@Shear Rate 1000 - 1000 1/s
Average value: 150000 cP Grade Count:1
Linear Mold Shrinkage 0.00200 - 0.0210 cm/cmAverage value: 0.0133 cm/cm Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 25.0 - 100 MPaAverage value: 47.6 MPa Grade Count:7
Tensile Strength, Ultimate 27.0 - 150 MPaAverage value: 51.6 MPa Grade Count:7
Tensile Strength, Yield 9.00 - 50.0 MPaAverage value: 30.9 MPa Grade Count:8
Elongation at Break 4.50 - 370 %Average value: 92.5 % Grade Count:16
Elongation at Yield 5.00 - 32.0 %Average value: 19.2 % Grade Count:6
Modulus of Elasticity 0.400 - 1.90 GPaAverage value: 0.820 GPa Grade Count:12
Flexural Yield Strength 23.0 - 52.0 MPaAverage value: 33.7 MPa Grade Count:3
Flexural Modulus 0.500 - 6.75 GPaAverage value: 1.78 GPa Grade Count:6
Poissons Ratio 0.450 - 0.470Average value: 0.457 Grade Count:4
Izod Impact, Notched 0.290 - 0.850 J/cmAverage value: 0.647 J/cm Grade Count:3
Izod Impact, Notched (ISO) 10.1 - 92.0 kJ/m²Average value: 48.8 kJ/m² Grade Count:3
 13.0 - 13.0 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 13.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 1000 - 2100 J/cm²Grade Count:9
 10.08 - 2099.79 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 10.1 J/cm² Grade Count:9
Charpy Impact, Notched 1.60 - 2100 J/cm²Average value: 5.52 J/cm² Grade Count:12
 1.092 - 7.98 J/cm²
@Temperature -40.0 - -30.0 °C
Average value: 2.13 J/cm² Grade Count:12
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+10 - 1.00e+13 ohm-cmAverage value: 1.40e+12 ohm-cm Grade Count:8
Surface Resistance 1.00e+10 - 1.00e+11 ohmAverage value: 5.50e+10 ohm Grade Count:4
Dielectric Strength 35.0 - 37.0 kV/mmAverage value: 36.0 kV/mm Grade Count:8
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:4
 
Thermal PropertiesOriginal ValueComments
CTE, linear 101 - 250 µm/m-°CAverage value: 181 µm/m-°C Grade Count:5
CTE, linear, Transverse to Flow 101 - 198 µm/m-°CAverage value: 132 µm/m-°C Grade Count:5
Melting Point 135 - 218 °CAverage value: 200 °C Grade Count:12
Maximum Service Temperature, Air 120 - 150 °CAverage value: 143 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 151 °CAverage value: 96.6 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 180 °CAverage value: 63.7 °C Grade Count:11
Flammability, UL94 HBGrade Count:4
Flame Spread 80.0 mm/minAverage value: 80.0 mm/min Grade Count:5
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 280 °CAverage value: 244 °C Grade Count:5
Drying Temperature 75.0 - 80.0 °CAverage value: 77.9 °C Grade Count:5
Moisture Content 0.0600 %Average value: 0.0600 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 11, Unreinforced
Overview of materials for Nylon 66, Impact Grade
Overview of materials for Nylon 610
Overview of materials for Nylon 6, 10% Glass Fiber Filled

O2601 / 78046

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.