MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 610
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.930 - 3.80 g/cc0.0336 - 0.137 lb/in³Average value: 1.26 g/cc Grade Count:265
Filler Content 15.0 - 50.0 %15.0 - 50.0 %Average value: 28.9 % Grade Count:41
Water Absorption 0.100 - 4.80 %0.100 - 4.80 %Average value: 1.45 % Grade Count:127
Moisture Absorption at Equilibrium 0.100 - 1.80 %0.100 - 1.80 %Average value: 0.703 % Grade Count:86
 0.900 - 1.70 %
@Temperature 70.0 - 70.0 °C
0.900 - 1.70 %
@Temperature 158 - 158 °F
Average value: 1.27 % Grade Count:18
Water Absorption at Saturation 0.350 - 6.00 %0.350 - 6.00 %Average value: 2.68 % Grade Count:53
 0.400 - 1.20 %
@Temperature 45.0 - 400 °C
0.400 - 1.20 %
@Temperature 113 - 752 °F
Average value: 0.814 % Grade Count:2
 0.400 - 1.20 %
@Treatment Temp. 70.0 - 70.0 °C
0.400 - 1.20 %
@Treatment Temp. 158 - 158 °F
Average value: 0.814 % Grade Count:2
Additive Loading 10.0 - 40.0 %10.0 - 40.0 %Average value: 24.5 % Grade Count:4
Viscosity 360000 - 360000 cP
@Temperature 250 - 250 °C
360000 - 360000 cP
@Temperature 482 - 482 °F
Average value: 301000 cP Grade Count:1
 0.200 - 1.30e+6 cP
@Temperature 230 - 300 °C
0.200 - 1.30e+6 cP
@Temperature 446 - 572 °F
Average value: 301000 cP Grade Count:8
 0.200 - 1.30e+6 cP
@Shear Rate 10.0 - 8000 1/s
0.200 - 1.30e+6 cP
@Shear Rate 10.0 - 8000 1/s
Average value: 301000 cP Grade Count:8
Viscosity Test 130 - 150 cm³/g1.30 - 1.50 dl/gAverage value: 148 cm³/g Grade Count:11
Viscosity Number 145 - 220 cm³/g1.45 - 2.20 dl/gAverage value: 171 cm³/g Grade Count:7
Linear Mold Shrinkage 0.000600 - 0.0510 cm/cm0.000600 - 0.0510 in/inAverage value: 0.00769 cm/cm Grade Count:193
Linear Mold Shrinkage, Transverse 0.00100 - 0.0790 cm/cm0.00100 - 0.0790 in/inAverage value: 0.0131 cm/cm Grade Count:129
Melt Flow 4.00 - 130 g/10 min4.00 - 130 g/10 minAverage value: 39.8 g/10 min Grade Count:17
Spiral Flow 35.0 - 700 cm13.8 - 276 inAverage value: 110 cm Grade Count:10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112 - 122112 - 122Average value: 118 Grade Count:15
Hardness, Shore D 63.0 - 84.063.0 - 84.0Average value: 73.3 Grade Count:4
Ball Indentation Hardness 25.0 - 245 MPa3630 - 35500 psiAverage value: 112 MPa Grade Count:51
Tensile Strength, Ultimate 20.0 - 1330 MPa2900 - 193000 psiAverage value: 127 MPa Grade Count:217
 25.0 - 155 MPa
@Temperature -40.0 - 150 °C
3630 - 22500 psi
@Temperature -40.0 - 302 °F
Average value: 97.0 MPa Grade Count:3
Tensile Strength, Yield 24.0 - 193 MPa3480 - 28000 psiAverage value: 82.8 MPa Grade Count:66
Elongation at Break 0.500 - 300 %0.500 - 300 %Average value: 28.1 % Grade Count:231
 3.30 - 6.10 %
@Temperature 60.0 - 150 °C
3.30 - 6.10 %
@Temperature 140 - 302 °F
Average value: 36.4 % Grade Count:3
Elongation at Yield 1.60 - 100 %1.60 - 100 %Average value: 10.8 % Grade Count:66
Modulus of Elasticity 0.350 - 27.6 GPa50.8 - 4000 ksiAverage value: 6.83 GPa Grade Count:224
 0.200 - 9.80 GPa
@Temperature 60.0 - 150 °C
29.0 - 1420 ksi
@Temperature 140 - 302 °F
Average value: 4.05 GPa Grade Count:3
Tenacity 0.370 - 0.509 N/tex4.19 - 5.77 g/denierAverage value: 0.447 N/tex Grade Count:3
Flexural Yield Strength 15.0 - 393 MPa2180 - 57000 psiAverage value: 196 MPa Grade Count:131
Flexural Modulus 0.120 - 22.1 GPa17.4 - 3200 ksiAverage value: 7.10 GPa Grade Count:153
 0.500 - 2.30 GPa
@Temperature -40.0 - 80.0 °C
72.5 - 334 ksi
@Temperature -40.0 - 176 °F
Average value: 1.40 GPa Grade Count:1
Flexural Strain at Break 3.60 - 5.50 %3.60 - 5.50 %Average value: 5.09 % Grade Count:6
Compressive Yield Strength 65.0 - 179 MPa9430 - 26000 psiAverage value: 136 MPa Grade Count:7
Poissons Ratio 0.340 - 0.4600.340 - 0.460Average value: 0.403 Grade Count:13
Shear Strength 45.0 - 79.0 MPa6530 - 11500 psiAverage value: 60.3 MPa Grade Count:5
Secant Modulus  0.901953 - 10.9027 GPa
@Temperature -40.0 - 100 °C
130.819 - 1581.33 ksi
@Temperature -40.0 - 212 °F
Average value: 5.67 GPa Grade Count:1
 0.901953 - 10.9027 GPa
@Strain 0.190 - 10.2 %
130.819 - 1581.33 ksi
@Strain 0.190 - 10.2 %
Average value: 5.67 GPa Grade Count:1
Izod Impact 29.0 - 603 J21.4 - 445 ft-lbAverage value: 134 J Grade Count:20
Izod Impact, Notched 0.366 - 6.67 J/cm0.685 - 12.5 ft-lb/inAverage value: 1.16 J/cm Grade Count:70
Izod Impact, Unnotched 3.67 - 5340 J/cm6.88 - 10000 ft-lb/inAverage value: 8.93 J/cm Grade Count:53
Izod Impact, Notched (ISO) 1.00 - 88.2 kJ/m²0.476 - 42.0 ft-lb/in²Average value: 13.4 kJ/m² Grade Count:41
 4.40 - 20.0 kJ/m²
@Temperature -40.0 - -30.0 °C
2.09 - 9.52 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 9.13 kJ/m² Grade Count:8
Izod Impact, Unnotched (ISO) 4.00 - 21000 kJ/m²1.90 - 9990 ft-lb/in²Average value: 61.5 kJ/m² Grade Count:32
 89.0 - 92.0 kJ/m²
@Temperature -30.0 - -30.0 °C
42.4 - 43.8 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 90.3 kJ/m² Grade Count:3
Charpy Impact Unnotched 3.00 - 2100 J/cm²14.3 - 9990 ft-lb/in²Average value: 8.73 J/cm² Grade Count:137
 4.50 J/cm² - NB
@Temperature -40.0 - -20.0 °C
21.4 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 9.03 J/cm² Grade Count:94
Charpy Impact, Notched 0.300 - 2100 J/cm²1.43 - 9990 ft-lb/in²Average value: 1.89 J/cm² Grade Count:132
 0.300 - 11.0 J/cm²
@Temperature -40.0 - -20.0 °C
1.43 - 52.4 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.53 J/cm² Grade Count:102
Gardner Impact 4.63 - 36.2 J3.42 - 26.7 ft-lbAverage value: 25.6 J Grade Count:3
Dart Drop, Total Energy 3.00 - 11.0 J2.21 - 8.11 ft-lbAverage value: 6.92 J Grade Count:13
Falling Dart Impact 8.50 - 11.8 J6.27 - 8.70 ft-lbAverage value: 9.88 J Grade Count:4
Instrumented Impact Total Energy 2.72 - 4.76 J2.01 - 3.51 ft-lbAverage value: 3.55 J Grade Count:4
Coefficient of Friction 0.260 - 0.7100.260 - 0.710Average value: 0.484 Grade Count:9
Coefficient of Friction, Static 0.100 - 0.5200.100 - 0.520Average value: 0.373 Grade Count:9
K (wear) Factor 8.06 - 894 x 10-8 mm³/N-M4.00 - 444 x 10-10 in³-min/ft-lb-hrAverage value: 125 x 10-8 mm³/N-M Grade Count:9
Taber Abrasion, mg/1000 Cycles 4.00 - 6.004.00 - 6.00Average value: 5.67 Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.00 - 1.00e+16 ohm-cm5.00 - 1.00e+16 ohm-cmAverage value: 3.55e+14 ohm-cm Grade Count:93
Surface Resistance 10.0 - 1.00e+15 ohm10.0 - 1.00e+15 ohmAverage value: 2.28e+13 ohm Grade Count:47
Dielectric Constant 3.10 - 3.903.10 - 3.90Average value: 3.61 Grade Count:7
Dielectric Strength 5.00 - 45.0 kV/mm127 - 1140 kV/inAverage value: 35.0 kV/mm Grade Count:57
Dissipation Factor 0.0140 - 0.04000.0140 - 0.0400Average value: 0.0270 Grade Count:5
Comparative Tracking Index 450 - 600 V450 - 600 VAverage value: 593 V Grade Count:41
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.40 - 200 µm/m-°C4.11 - 111 µin/in-°FAverage value: 68.7 µm/m-°C Grade Count:74
 18.0 - 100 µm/m-°C
@Temperature 35.0 - 55.0 °C
10.0 - 55.6 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 59.0 µm/m-°C Grade Count:2
 18.0 - 100 µm/m-°C
@Thickness 2.00 - 2.00 mm
10.0 - 55.6 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 59.0 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 48.0 - 170 µm/m-°C26.7 - 94.4 µin/in-°FAverage value: 102 µm/m-°C Grade Count:60
Specific Heat Capacity 1.90 - 2.28 J/g-°C0.454 - 0.545 BTU/lb-°FAverage value: 2.13 J/g-°C Grade Count:5
Thermal Conductivity 0.250 - 0.562 W/m-K1.74 - 3.90 BTU-in/hr-ft²-°FAverage value: 0.359 W/m-K Grade Count:8
Melting Point 156 - 262 °C313 - 504 °FAverage value: 221 °C Grade Count:153
Maximum Service Temperature, Air 70.0 - 220 °C158 - 428 °FAverage value: 138 °C Grade Count:35
Deflection Temperature at 0.46 MPa (66 psi) 50.0 - 232 °C122 - 450 °FAverage value: 181 °C Grade Count:102
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 227 °C104 - 440 °FAverage value: 154 °C Grade Count:170
Deflection Temperature at 8.0 MPa 75.0 - 190 °C167 - 374 °FAverage value: 135 °C Grade Count:25
Vicat Softening Point 180 - 221 °C356 - 430 °FAverage value: 211 °C Grade Count:17
Glass Transition Temp, Tg 42.0 - 73.0 °C108 - 163 °FAverage value: 55.2 °C Grade Count:16
UL RTI, Electrical 65.0 °C149 °FAverage value: 65.0 °C Grade Count:7
UL RTI, Mechanical with Impact 65.0 °C149 °FAverage value: 65.0 °C Grade Count:7
UL RTI, Mechanical without Impact 65.0 °C149 °FAverage value: 65.0 °C Grade Count:7
Flammability, UL94 HB - V-0HB - V-0Grade Count:102
Flame Spread 80.0 mm/min3.15 in/minAverage value: 80.0 mm/min Grade Count:9
Oxygen Index 24.0 - 25.0 %24.0 - 25.0 %Average value: 24.7 % Grade Count:3
 
Optical PropertiesMetricEnglishComments
Yellow Index 8.00 %8.00 %Average value: 8.00 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 215 - 295 °C419 - 563 °FAverage value: 279 °C Grade Count:20
Nozzle Temperature 240 - 310 °C464 - 590 °FAverage value: 275 °C Grade Count:12
Die Temperature 210 - 270 °C410 - 518 °FAverage value: 235 °C Grade Count:6
Melt Temperature 50.0 - 310 °C122 - 590 °FAverage value: 267 °C Grade Count:124
Mold Temperature 8.00 - 120 °C46.4 - 248 °FAverage value: 84.3 °C Grade Count:122
Drying Temperature 70.0 - 120 °C158 - 248 °FAverage value: 81.3 °C Grade Count:96
Moisture Content 0.0200 - 0.250 %0.0200 - 0.250 %Average value: 0.152 % Grade Count:51
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:14
Injection Pressure 68.9 - 130 MPa10000 - 18900 psiAverage value: 96.6 MPa Grade Count:31

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Overview of materials for Nylon 612, Unreinforced
Overview of materials for Nylon 11, Unreinforced
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 6, Unreinforced

O2590 / 77792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.