MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
Categories: Ceramic; Ceramic Matrix Composite

Material Notes: RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for performance sensitive, high volume commercial applications. RO4000 laminates are designed to offer superior high frequency performance and low-cost circuit fabrication. The result is a low loss material which can be fabricated using standard epoxy/glass (FR4) processes.

Features and Benefits:

  • Glass-reinforced hydrocarbon and ceramic dielectric
  • Volume manufacturing process
  • Excellent high-frequency performance
  • Low Z-axis expansion, excellent dimensional stability
  • Integrated thin film resistor benefits
  • Foils available in 25, 50 and 100 OPS NiCr
  • Foils offered in 1/2 ounce copper weight
  • Lead-Free process compatible

Typical Applications:

  • Global communications systems
  • High reliability and complex multilayer circuits
  • Wireless communication devices

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.86 g/ccASTM D792
Moisture Absorption at Equilibrium 0.060 %
@Temperature 50.0 °C,
Time 173000 sec
Immersion; 0.06 in thick; ASTM D570
Thickness 6.60 - 60.0 milRange of Thicknesses Available
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25400 psiRT, Y direction; ASTM D638
Tensile Modulus 1664 ksiRT, Y direction; ASTM D638
Flexural Strength 255 MPaIPC-TM-650, 2.4.4
Peel Strength 5.00 pliCopper, After Solder Float, 1/2 ounce TCR Foil; IPC-TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+16 ohm-cmCond. A; IPC 2.5.17.1
Surface Resistance 5.70e+15 ohmCond. A; IPC 2.5.17.1
Dielectric Constant 3.66Design Spec., FSR, Z-direction; IPC-TM-650 2.5.5.6
 3.43 - 3.53
@Frequency 1e+10 Hz
Process, Clamped stripline, Z-direction; IPC-TM-650 2.5.5.5
Dielectric Strength 780 V/mil
@Thickness 0.510 mm
Z Direction; IPC-TM-650 2.5.6.2
Dissipation Factor 0.0031
@Frequency 2.50e+9 Hz
IPC-TM-650 2.5.5.5
 0.0037
@Frequency 1e+10 Hz
IPC-TM-650 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature -55.0 - 288 °C
X-Direction; IPC-TM-650 2.4.41
 16.0 µm/m-°C
@Temperature -55.0 - 288 °C
Y-Direction; IPC-TM-650 2.4.41
 35.0 µm/m-°C
@Temperature -55.0 - 288 °C
Z-Direction; IPC-TM-650 2.4.41
Thermal Conductivity 0.690 W/m-K
@Temperature 80.0 °C
ASTM C518
Glass Transition Temp, Tg >= 280 °CCondition A; IPC-TM-650 2.4.24
Decomposition Temperature 390 °CTGA; ASTM D3850
Flammability, UL94 V-0
 
Descriptive Properties
Dimensional Stability< 0.5 mm/mX, Y direction; IPC-TM-650, 2.4.39A; after etch; +E2/150°C
Thermal Coefficient of Dielectric Constant50 ppm/°CIPC-TM-650 2.5.5.5; -50°C to 150°C; Z-Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arlon Electronic Materials 25FR Low-Cost Ceramic Hydrocarbon
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil
Silicon Carbide, Reaction-Bonded, SiSiC
AISI 8620 Steel, normalized, 13 mm (0.5 in.) round

PROGA955 / 138395

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.