MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products Kwik Kast BC 8650 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittle parts. Designed for constructing patterns, prototypes, duplications, negatives, low temperature vacuum form tools, tracing models, etc.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 g/cc
Brookfield Viscosity 2360 cP
@Temperature 23.9 °C
1 minute
Linear Mold Shrinkage 0.00080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81 - 85
@Temperature 23.9 °C
Tensile Strength, Ultimate 4120 psi
Flexural Strength 6250 psi
Compressive Strength 9200 psi
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 120 min
@Temperature 24.0 °C
demold time
Pot Life 5.0 - 6.0 min
@Temperature 24.0 °C
1 lb. mass
 
Descriptive Properties
Mix Ratio1:1 by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products Kwik Kast BC 8645 Urethane Casting
BCC Products METAL-KAST BC 8010 Urethane Casting
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting
BCC Products SLO-KAST BC 8009 Urethane Casting
BCC Products BC 8870 Polyurethane Elastomer

PBCC049 / 107276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.