MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products METAL-KAST BC 8010 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to premix due to less settling. New BC8010 exhibits good heat transfer properties and is ideally suited for a multitude of applications, to include construction of short run low temperature vacuum form tools, prototypes, models, display parts, fixturing and bulk back fill.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 1.85 g/cc1.75 - 1.85 g/cc
Brookfield Viscosity 2250 cP
@Temperature 23.9 °C
2250 cP
@Temperature 75.0 °F
1 minute, #3 spindle @ 20 rpm
Linear Mold Shrinkage 0.00070 cm/cm0.00070 in/inASTM D2566-69
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 83
@Temperature 23.9 °C
83
@Temperature 75.0 °F
Tensile Strength, Ultimate 27.90 MPa4046 psiASTM D638
Flexural Strength 45.9 MPa6650 psiASTM D790
Compressive Strength 67.2 MPa9750 psiASTM D695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 81.7 °C179 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 - 120 min
@Temperature 24.0 °C
1.50 - 2.00 hour
@Temperature 75.2 °F
demold time
Pot Life 6.0 - 7.0 min
@Temperature 24.0 °C
6.0 - 7.0 min
@Temperature 75.2 °F
1 lb. mass
 
Descriptive Properties
Mix Ratio1:1 by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products Kwik Kast BC 8645 Urethane Casting
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting
BCC Products Kwik Kast BC 8650 Urethane Casting
BCC Products SLO-KAST BC 8009 Urethane Casting
BCC Products BC 8870 Polyurethane Elastomer

PBCC047 / 107274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.