MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products SLO-KAST BC 8009 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user longer working time for filling large closed mold cavities. Slo-Kast is ideal for casting large sections without having to stage pour. Uses include; tracing models, core boxes, keller aids, patterns, core sticks, vacuum form tools, prototypes and display parts.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 1.90 g/cc1.80 - 1.90 g/ccASTM D792-66
Brookfield Viscosity 2950 cP
@Temperature 23.9 °C
2950 cP
@Temperature 75.0 °F
#3 spindle @ 20 rpm; ASTM D2393
Linear Mold Shrinkage 0.00020 cm/cm0.00020 in/inASTM D2566-69
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85
@Temperature 23.9 °C
85
@Temperature 75.0 °F
ASTM D2240
Tensile Strength, Ultimate 40.3 MPa5850 psi
Compressive Strength 60.7 MPa8800 psiASTM D695
 
Processing PropertiesMetricEnglishComments
Cure Time 210 - 240 min
@Temperature 24.0 °C
3.50 - 4.00 hour
@Temperature 75.2 °F
demold time
Pot Life 14 - 17 min
@Temperature 24.0 °C
14 - 17 min
@Temperature 75.2 °F
1 lb. mass
 
Descriptive Properties
Mix Ratio1:1 by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products Kwik Kast BC 8002 Urethane Casting
BCC Products Kwik Kast BC 8645 Urethane Casting
BCC Products Kwik Kast BC 8650 Urethane Casting
BCC Products METAL-KAST BC 8010 Urethane Casting
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting

PBCC045 / 107272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.