MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SIDPEC EGYPTENE® HD 5301 FB HDPE Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Applications:
  • Strong thin film
  • Carrier bag
  • Grocery sacks

Film properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.

Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³ISO 1872/1
Thickness 15.0 microns0.591 mil
Melt Flow 0.050 g/10 min
@Load 2.16 kg
0.050 g/10 min
@Load 4.76 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 32.0 MPa4640 psiISO 1184
Film Tensile Strength at Yield, TD 29.0 MPa4210 psiISO 1184
Film Elongation at Break, MD 450 %450 %ISO 1184
Film Elongation at Break, TD 400 %400 %ISO 1184
Dart Drop 10.0 g/micron254 g/milCalculated from thickness
Dart Drop Test 150 g0.331 lbASTM D1709
Film Tensile Strength at Break, MD 56.0 MPa8120 psiISO 1184
Film Tensile Strength at Break, TD 65.0 MPa9430 psiISO 1184

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding
ExxonMobil HD 7957.04 High Density Polyethylene (HDPE), Film Grade
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
ExxonMobil HMA 025 High Density Polyethylene Resin

PSIDP00 / 67695

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.