MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.

Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The high stiffness combined with good optical properties brings a significant down-gauging potential.

Lumicene® mPE M 6040 S01 is a versatile resin that can be used in pure or in blend for the production of both monolayer and multilayer film. Typical applications are: specialty film, hygiene film, embossed film, compounds and consumer and automatic packaging, such as produce bags, mailing and overwrap film. The high density of Lumicene® mPE M 6040 S01 enables its use in applications with moisture barrier requirements, such as dry food packaging, and brings improved heat resistance, compared to commonly used HDPE.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccISO 1183
Thickness 20.0 microns0.787 mil
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 23.0 MPa3340 psiISO 527-3
Film Tensile Strength at Yield, TD 24.0 MPa3480 psiISO 527-3
Film Elongation at Break, MD 520 %520 %ISO 527-3
Film Elongation at Break, TD 850 %850 %ISO 527-3
Elmendorf Tear Strength, MD 0.800 g/micron20.3 g/milISO 6383-2
Elmendorf Tear Strength, TD 7.10 g/micron180 g/milISO 6383-2
Dart Drop Test 40.0 g0.0882 lbISO 7765-1
Film Tensile Strength at Break, MD 26.0 MPa3770 psiISO 527-3
Film Tensile Strength at Break, TD 34.0 MPa4930 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 134 °C273 °FISO 11357
Vicat Softening Point 132 °C270 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ISO 14782
Gloss 51 %51 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 80.0 °C68.0 - 176 °FChill Roll
Melt Temperature 220 - 280 °C428 - 536 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film

PTOTAL785 / 130510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.