MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 6001 High Density Polyethylene (HDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: ExxonMobil™ HD 6001 is a high molecular weight HDPE film resin. Films made with ExxonMobil™ HD 6001 exhibit excellent tensile properties, aswell as high stiffness. ExxonMobil™ HD 6001 is particularly suited for draw tape applications

Availability:  Latin America, North America.  Applications: draw tape.

Information provided by ExxonMobil.

Key Words: HDPE HD 7957.04
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³ASTM D1505
Thickness 25.4 microns1.00 miltested
Melt Flow 0.060 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.060 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ExxonMobil correlation; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 41.4 MPa6000 psiASTM D882
Film Tensile Strength at Yield, TD 35.9 MPa5200 psiASTM D882
Film Elongation at Break, MD 310 %310 %ASTM D882
Film Elongation at Break, TD 380 %380 %ASTM D882
Elmendorf Tear Strength MD 9.0 g9.0 gASTM D1922
Elmendorf Tear Strength TD 20 g20 gASTM D1922
Dart Drop Test 280 g0.617 lbASTM D1709A
Film Tensile Strength at Break, MD 89.6 MPa13000 psiASTM D882
Film Tensile Strength at Break, TD 75.8 MPa11000 psiASTM D882
1% Secant Modulus, MD 1240 MPa180000 psiASTM D882
1% Secant Modulus, TD 1240 MPa180000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C272 °F
Crystallization Temperature 119 °C246 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene

PEX98883 / 238265

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.