MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Glyptal 7815 Black Enamel
Categories: Polymer; Thermoset; Alkyd

Material Notes: GLYPTAL 7815 GLOSS BLACK ENAMEL is a fast air-drying or low-temperature bake finish. This product is designed for use as a black, gloss finish coat on motor end windings and electrical equipment. This paint is compatible with most insulating systems. It has excellent oil, humidity and weather resistance. 7815 can be used in areas where some exterior durability is required along with fast-drying properties.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.26 - 10.3 lb/gal
 13.74 - 13.78 lb/galSolid
Solids Content 36 - 38 %Volume
 43 - 45 %Weight
Thickness 1.00 - 1.50 milDry Film
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 80.0 °Fcc/pm
 
Optical PropertiesOriginal ValueComments
Gloss >= 80 %60°
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hourTackfree
 2.00 - 3.00 hourDry to Handle
 12.0 hourHard
 
Descriptive Properties
Adhesion1Cross Hatch
Bake Time45 mins150°F
ColorBlack
Coverage600 ft²/gal
MethodSpray
Oil ResistantExcellent
ReducerG-1500
SubstrateCRS
Viscosity25-30 secondsReduced; #2 Zahn

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Glyptal 8001 Insulating Enamel
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Silicone Polyurethane, Ether Based
Glyptal G1228 High-Gloss Enamel

PGLYPT912 / 209751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.