MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Glyptal 8001 Insulating Enamel
Categories: Polymer; Thermoset; Alkyd

Material Notes: GLYPTAL 8001 is a red, insulating enamel that can be air-dried or baked. Films of this paint have excellent humidity and salt water resistance as well as dielectric strength. Glyptal 8001 Red offers good heat aging properties and oil resistance. This paint is not suitable for the inside coating of dielectric oil containers.

SUGGESTED USES

Glyptal 8001 is suggested for coating motor stators, field coils, end windings, bus bars, and switch bases. It adheres well to molded phenolics and phenolic varnish films. This paint can also be used as a metal primer where some degree of corrosion resistance is needed.

APPLICATION

Glyptal 8001 Red Enamel is designed for use by spray, dip, or flow coat. For best results apply on clean, dry surfaces at temperatures above 50 ºF.

Reduction:

Spray- Reduce with 1500 Thinner to a viscosity of 24-28 seconds (#2 Zahn Cup)

Dip or Flow- Reduce with Aromatic 100 to a viscosity of 30-35 seconds (#2 Zahn Cup)

SURFACE PREPARATION

Surface to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove all grease and oil by washing surface with mineral spirits.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.646 - 1.651 g/cc0.05948 - 0.05965 lb/in³
Solids Content 56 - 59 %56 - 59 %Weight
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 66.9 kV/mm1700 kV/inASTM D115-55
Arc Resistance 30 sec30 secon Textolite
 
Thermal PropertiesMetricEnglishComments
Flash Point <= 26.7 °C<= 80.0 °Fcc/pm
 
Processing PropertiesMetricEnglishComments
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourAir Dry, Touch
 12.0 hour12.0 hourAir Dry: Hard
 12.0 hour12.0 hourAir Dry: Recoat
 
Descriptive Properties
Bake Time1-3 hr335-375°F
ColorIron Oxide Red
Coverage650 ft²/gal
Viscosity80-85 KU

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Glyptal 7815 Black Enamel
Wacker Silres® SY 300 Silicone Intermediate
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Silicone Polyurethane, Ether Based

PGLYPT914 / 209753

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.